Suke Plastics 1045 PC ABS

suke plastics resin raw material granules 25kg package

Suke 1045 PC/ABS Resin General Purpose Grade

Suke 1045 is a versatile general-purpose PC/ABS resin engineered for reliability across demanding applications. Combining excellent mechanical strength, ease of processing, and balanced thermal stability, it delivers consistent performance for industrial and consumer components. Ideal for electronics and office equipment where durability matters.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Density: 1.10 g/cm³ (ASTM D792, 23°C)
  • Mold Shrinkage: 0.4–0.7% (ASTM D955, 2 mm)
Mechanical Properties
  • Tensile Strength: 51 MPa (ASTM D638, 50 mm/min)
  • Elongation at Break: 35% (ASTM D638, 50 mm/min)
  • Flexural Strength: 72 MPa (ASTM D790, 2 mm/min)
  • Flexural Modulus: 2200 MPa (ASTM D790, 2 mm/min)
Impact Properties

IZOD Notched Impact Strength: 50 KJ/m² (ASTM D256, 3.2 mm, 23°C)

Thermal Properties

Heat Distortion Temperature (HDT): 92°C (ASTM D648, 1.8 MPa, 3.2 mm)

Flame Characteristics

Flammability Rating: Class / (UL94, 3.2 mm)

Injection Molding
  • Pre-drying Condition: 85–95°C, 3 hours
  • Injection Pressure: 60–100 MPa
  • Injection Speed: 50–80
  • Mold Temperature: 80°C
  • Processing Temperature (Max): 270°C
  • Melt Temperature: 250°C
  • Cylinder Temperatures:
    • Feeding: 220–240°C
    • Compressing: 230–250°C
    • Nozzle: 240–260°C

Features & Benefits

Robust Mechanical Integrity

With 45 MPa tensile strength and 45 KJ/m² impact resistance, Suke plastic PC 1045 withstands drops and stresses—perfect for protective casings and structural parts in rugged environments.

Streamlined Processing

A melt flow rate of 22 g/10min (260°C) ensures smooth injection molding, reducing cycle times and energy costs while maintaining dimensional stability (0.4–0.7% shrinkage).

Balanced Thermal Resistance

It survives up to 86°C under load, making Suke 1045 reliable for heat-exposed components like printer housings or power tool grips without warping.

suke 1045 pc abs resin

Use & Applications

  • Electrical & Electronics: Durable connectors, power tool housings, and appliance components.
  • Office Supplies: Printer frames, computer accessories, and ergonomic device casings.
suke 1045 pc abs plastic application