Suke Plastics 1065 PC ABS

suke plastics resin raw material granules 25kg package

Suke 1065 PC/ABS Resin General Purpose Grade

Suke 1065 is a high-performance, general-purpose PC/ABS resin offering exceptional balance. Its good comprehensive performance combines the strength of Polycarbonate (PC) with the processability of Acrylonitrile Butadiene Styrene (ABS), making it ideal for demanding applications across electronics and office equipment. Experience reliability and ease of manufacturing.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Density: 1.14 g/cm³ (ASTM D792, 23°C)
  • Mold Shrinkage: 0.4–0.7% (Internal, 2mm)
Mechanical Properties
  • Tensile Strength: 57 MPa (ASTM D638, 50mm/min)
  • Elongation at Break: 50% (ASTM D638, 50mm/min)
  • Flexural Strength: 75 MPa (ASTM D790, 2mm/min)
  • Flexural Modulus: 2200 MPa (ASTM D790, 2mm/min)
Impact Properties

Impact Strength (IZOD Notched): 55 KJ/m² (ASTM D256, 3.2mm, 23°C)

Thermal Properties

Heat Distortion Temperature (HDT): 103°C (ASTM D648, 1.8MPa, 3.2mm)

Flame Characteristics

Flammability: UL94 Class (3.2mm)

Injection Molding
  • Pre-drying Condition: 90°C–100°C, 3 hours
  • Injection Pressure: 60–100 MPa
  • Injection Speed: 50–80
  • Mold Temperature: 80°C
  • Processing Temperature (Max): 280°C
  • Melt Temperature: 260°C
  • Cylinder Temperature – Feeding Zone: 230°C–250°C
  • Cylinder Temperature – Compression Zone: 240°C–260°C
  • Cylinder Temperature – Nozzle Zone: 250°C–270°C

Features & Benefits

Impact Strength You Can Trust

Suke 1065 delivers excellent toughness (55 KJ/m² IZOD notched), minimizing part breakage during assembly, drops, or everyday use. This reliability is crucial for durable electronic housings and office machinery components.

Balanced Strength & Stiffness

It achieve robust parts with good tensile strength (57 MPa) and stiffness (2200 MPa flexural modulus). This balance ensures structural integrity for components like computer bezels, printer parts, and tool housings without excessive weight.

Streamlined Production Efficiency

With a high melt flow rate (22 g/10min) and clear processing guidelines, Suke 1065 fills molds quickly and consistently. Reduced cycle times and predictable behavior lower manufacturing costs and complexity.

suke 1065 pc abs resin

Use & Applications

  • Electrical & Electronic (E&E): Computer monitor bezels and housings; Printer and copier exteriors and internal components; Power tool housings; Consumer electronics enclosures; Electrical connectors and sockets.
  • Office Supplies: Durable casings for staplers, hole punches, tape dispensers; Frames and bodies for desktop organizers; Components for projectors and presentation equipment; Robust housings for calculators and electronic office devices.
suke 1065 pc abs plastic application