Suke 3016GL PC/ABS Resin Flame Retardant Grade

Suke 3016GL is a halogen-free PC/ABS solution offering exceptional high fluidity for complex, thin-walled components. Engineered for demanding electrical, electronic, and consumer applications, it delivers reliable V0 flame retardancy, balanced toughness, and excellent processability, streamlining your production while meeting critical safety standards.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Density: 1.18 g/cm³ (ASTM D792, 23°C)
  • Mold Shrinkage: 0.4–0.8% (Internal Standard, 2 mm)
Mechanical Properties
  • Tensile Strength: 50 MPa (ASTM D638, 50 mm/min)
  • Elongation at Break: 30% (ASTM D638, 50 mm/min)
  • Flexural Strength: 90 MPa (ASTM D790, 2 mm/min)
  • Flexural Modulus: 2100 MPa (ASTM D790, 2 mm/min)
Impact Properties

Izod Notched Impact Strength: 50 kJ/m² (ASTM D256, 3.2 mm, 23°C)

Thermal Properties

Heat Distortion Temperature (HDT): 82°C (ASTM D648, 1.8 MPa, 6.4 mm)

Flame Characteristics

Flammability: UL94 Class V0 (1.5 mm)

Injection Molding
  • Pre-drying Conditions: 75–85°C for 3 hours
  • Injection Pressure: 60–100 MPa
  • Injection Speed: 50–80
  • Mold Temperature: 70°C
  • Melt Temperature: 250°C
  • Processing Temperature Max.: 270°C
  • Cylinder Temperature:
    • Feeding Zone: 220–240°C
    • Compression Zone: 230–250°C
    • Nozzle Zone: 240–260°C

Features & Benefits

Superior Flame Safety Guaranteed

Achieve UL94 V0 rating at just 1.5mm thickness. This halogen-free formulation ensures critical fire safety for electronics and enclosures without toxic smoke, protecting end-users and meeting stringent global regulations.

Exceptional Flow for Complex Designs

Leverage its high fluidity (MFR 30 g/10min) to effortlessly fill intricate molds and produce thin-walled parts. Reduce injection pressure, minimize warpage, shorten cycle times, and boost production efficiency.

Optimal Balance of Strength & Toughness

Benefit from robust mechanical properties – 50 MPa tensile strength and 50 KJ/m² impact strength. This balance ensures durable housings, connectors, and structural parts resist everyday impacts and stresses reliably.

suke 3016gl pc abs resin

Use & Applications

  • Electrical & Electronic Components: Housings for switches, connectors, sockets, power adapters, control boxes
  • Office Equipment & Supplies: Printer components, scanner housings, keyboard frames, monitor bezels
  • Networking Hardware: Router enclosures, modem casings, switch housings, and other telecom equipment parts