Suke 3016NH is a premium halogen-free PC/ABS resin engineered for demanding applications. Combining exceptional chemical resistance with robust mechanical performance, it delivers reliability for electronics, office equipment, and wearable tech—all while meeting strict environmental and safety standards.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Density: 1.18 g/cm³ (ASTM D792, 23°C)
  • Mold Shrinkage: 0.4–0.8% (Internal Standard, 2 mm)
Mechanical Properties
  • Tensile Strength: 55 MPa (ASTM D638, 50 mm/min)
  • Flexural Strength: 85 MPa (ASTM D790, 2 mm/min)
  • Flexural Modulus: 2000 MPa (ASTM D790, 2 mm/min)
  • Elongation at Break: 50% (ASTM D638, 50 mm/min)
Impact Properties

Impact Strength (Izod, Notched): 60 kJ/m² (ASTM D256, 3.2 mm, 23°C)

Thermal Properties

Heat Distortion Temperature: 88°C (ASTM D648, 1.8 MPa, 6.4 mm)

Flame Characteristics

Flammability: UL94 V-0 (1.5 mm)

Injection Molding
  • Pre-drying Conditions: 80–90°C for 3 hours
  • Injection Pressure: 60–100 MPa
  • Injection Speed: 50–80 mm/s
  • Mold Temperature: 80°C
  • Processing Temperature:
    • Max: 280°C
    • Melt Temperature: 260°C
    • Cylinder Temperatures:
      • Feeding Zone: 230–250°C
      • Compressing Zone: 240–260°C
      • Nozzle: 250–270°C

Features & Benefits

Halogen-Free Safety

Ideal for eco-conscious manufacturing, this material eliminates toxic fumes during production or combustion, ensuring compliance with global environmental regulations (e.g., RoHS) for electronics and consumer goods.

Superior Chemical Resistance

It resists oils, solvents, and cleaning agents, preventing degradation in harsh environments—perfect for printer housings, electronic enclosures, and headset components exposed to daily wear.

Optimized Processing & Durability

With high flow (17g/10min MFR) and impact strength (60 KJ/m²), it enables easy molding of thin-walled parts while reducing cracks or failures in high-stress applications like headset hinges.

suke 3016nh pc abs resin

Use & Applications

  • Electrical & Electronic: Connectors, charger cases, power tool housings
  • Office Supplies: Printer components, keyboard frames, scanner covers
  • Bluetooth Headsets: Durable ear hooks, impact-resistant casings, hinges
suke 3016nh pc abs plastic application

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.