Physical Properties
- Density: 1.19 g/cm³ (ASTM D792, 23°C)
- Mold Shrinkage: 0.4–0.8% (ASTM D955, 2mm)
Mechanical Properties
- Tensile Strength: 55 MPa (ASTM D638, 50mm/min)
- Elongation at Break: 80% (ASTM D638, 50mm/min)
- Flexural Strength: 90 MPa (ASTM D790, 2mm/min)
- Flexural Modulus: 2200 MPa (ASTM D790, 2mm/min)
Impact Properties
Impact Strength (Izod Notched): 65 KJ/m² (ASTM D256, 3.2mm, 23°C)
Thermal Properties
Heat Distortion Temperature: 100°C (ASTM D648, 1.8Mpa, 6.4mm)
Flame Characteristics
Flammability Rating: UL94 V-0 (0.8mm thickness)
Injection Molding
- Pre-drying Condition: 90°C–95°C, 3 hours
- Injection Pressure: 60–100 MPa
- Injection Speed: 50–80
- Mold Temperature: 90°C
- Maximum Processing Temperature: 290°C
- Melt Temperature: 270°C
- Cylinder Temperature:
- Feeding Section: 240°C–260°C
- Compression Section: 250°C–270°C
- Nozzle: 260°C–280°C
Features & Benefits
Halogen-Free Safety Assurance
Suke 3020 eliminates toxic halogen emissions, ensuring eco-compliance and safer workplaces—critical for electronics manufacturing where material safety reduces regulatory risks.
Superior Flame Resistance
With UL94 V0 certification (0.8mm), it prevents fire propagation in high-heat environments like power adapters or server housings, minimizing product recalls and liability.
High Impact & Flow Efficiency
65 KJ/m² notched impact strength withstands drops/stress, while 10 g/10min MFR ensures easy molding of thin-walled parts (e.g., laptop bezels), cutting production cycles.
Use & Applications
- Electrical & Electronics: Charger housings, circuit breakers, server components.
- Office Supplies: Printer casings, keyboard frames, ergonomic device parts.