Suke Plastics 3040 PC ABS

suke plastics resin raw material granules 25kg package

Suke 3040 PC/ABS Resin Flame Retardant Grade

Suke 3040 is a halogen-free PC/ABS resin engineered for superior safety and versatile performance. Ideal for electronics, office gear, and POS terminals, it combines high impact resistance, flame retardancy (UL94 V0), and easy processability—perfect for durable, eco-conscious industrial applications.

Associated Documents

ASTM TDS
UL Product IQ

Typical property data

Physical Properties

Density: 1.18 g/cm³ (ASTM D792, at 23°C)

Mechanical Properties
  • Tensile Strength: 55 MPa (ASTM D638, at 50mm/min)
  • Elongation at Break: 50% (ASTM D638, at 50mm/min)
  • Flexural Strength: 88 MPa (ASTM D790, at 2mm/min)
  • Flexural Modulus: 2000 MPa (ASTM D790, at 2mm/min)
Impact Properties

Notched Izod Impact Strength: 60 KJ/m² (ASTM D256, at 3.2mm, 23°C)

Thermal Properties

Heat Deflection Temperature (HDT): 88°C (ASTM D648, at 1.8MPa, 6.4mm)

Flame Characteristics

Flammability Rating: V-0 (UL94, 1.5mm)

Injection Molding
  • Pre-Drying Condition: 80°C-90°C for 3 hours
  • Injection Pressure: 60-100 MPa
  • Mold Temperature: 80°C
  • Melt Temperature: 260°C
  • Maximum Processing Temperature: 280°C

Features & Benefits

Halogen-Free Safety

Suke 3040 eliminates toxic halogens, meeting strict environmental regulations. Use it in consumer electronics to reduce health risks and ensure safer end-of-life disposal—ideal for eco-certified products.

Balanced Strength & Toughness

With 55 MPa tensile strength and 60 KJ/m² impact resistance, it withstands drops and stress. Perfect for POS machine housings or office equipment that demands daily durability without cracking.

Flame-Retardant Reliability

It achieves UL94 V0 rating at 1.5mm thickness, ensuring fire safety in electrical enclosures. No extra additives needed—critical for compliance in high-risk public settings like retail terminals.

suke 3040 pc abs resin

Use & Applications

  • Electrical & Electronic: Power adapters, connectors, and device housings.
  • Office Supplies: Printer components, keyboard frames, and ergonomic tools.
  • POS Machines: Card readers, terminal casings, and retail kiosks.