Suke Plastics 5983 PC Resin

suke plastics resin raw material granules 25kg package

Suke 5983 PC Resin Flame Retardant Grade

Suke Plastics 5983 is an advanced halogen-free (chlorine & bromine free) polycarbonate resin engineered for exceptional impact strength and inherent flame retardancy (UL94 V0 @ 1.5mm). Perfectly suited for demanding electrical/electronic components and durable office equipment, it delivers safety, reliability, and ease of processing for high-quality parts.

Download PDF

UL Product IQ

Typical property data

Physical Properties
  • Density: 1.2 g/cm³ (ASTM D792, 23°C)
  • Mold Shrinkage: 0.5–0.7% (Internal Standard, 2 mm)
Mechanical Properties
  • Tensile Strength: 65 MPa (ASTM D638, 50 mm/min)
  • Elongation at Break: 100% (ASTM D638, 50 mm/min)
  • Flexural Strength: 88 MPa (ASTM D790, 2 mm/min)
  • Flexural Modulus: 2400 MPa (ASTM D790, 2 mm/min)
Impact Properties
  • Izod Notched Impact Strength: 70 kJ/m² (ASTM D256, 3.2 mm, 23°C)
Thermal Properties
  • Heat Deflection Temperature (HDT): 125°C (ASTM D648, 1.8 MPa, 6.4 mm)
Flame Characteristics
  • Flammability: V0 class (UL94, 1.5 mm)
Injection Molding
  • Pre-drying Conditions: 110–120°C for 4 hours
  • Injection Pressure: 60–100 MPa
  • Injection Speed: 50–80 mm/s
  • Mold Temperature: 100°C
  • Maximum Processing Temperature: 320°C
  • Melt Temperature: 280°C
  • Cylinder Temperature Ranges:
    • Feeding: 240–260°C
    • Compressing: 270–290°C
    • Nozzle: 280–300°C

Use & Applications

  • Electrical & Electronic Components: Connectors & housings; Switches and sockets; Protective covers and enclosures; Components requiring V0 flame safety.
  • Durable Office Supplies & Equipment: Printer & copier parts; Robust housings for electronic devices; High-stress components; Tool bodies.
suke 5983 pc plastic material application

Features & Benefits

Built-In Safety & Compliance

Its halogen-free formulation meets strict environmental regulations and safety standards for electronics and office products, reducing harmful emissions and ensuring responsible manufacturing.

Superior Impact Resistance

It boasts exceptionally high impact strength (70 KJ/m² IZOD notched). This means parts resist cracking or shattering from drops or impacts during assembly, shipping, or daily use.

Reliable Flame Retardancy

It achieves a UL94 V0 rating at thin walls (1.5mm), providing critical fire safety for sensitive electrical applications without compromising on material performance or requiring complex modifications.

suke 5983 pc resin