Plastic Granules
Suke D570 PC/ABS Resin General Purpose Grade
Suke D570 PC/ABS Resin delivers exceptional all-around performance for demanding industrial applications. This versatile engineering thermoplastic combines polycarbonate’s strength with ABS’s processability, offering balanced mechanical properties, ease of molding, and reliability for electronics, tools, and office equipment.
Associated Documents
ASTM TDS
Typical property data
Physical Properties
- Density: 1.07 g/cm³ (ASTM D792, 23°C)
- Mold Shrinkage: 0.4–0.7% (INTERNAL, 2 mm thickness)
Mechanical Properties
- Tensile Strength: 47 MPa (ASTM D638, 50 mm/min)
- Elongation at Break: 30% (ASTM D638, 50 mm/min)
- Flexural Strength: 70 MPa (ASTM D790, 2 mm/min)
- Flexural Modulus: 1900 MPa (ASTM D790, 2 mm/min)
Impact Properties
Impact Strength (IZOD Notched): 42 KJ/m² (ASTM D256, 3.2 mm thickness, 23°C)
Thermal Properties
Heat Deflection Temperature (HDT): 86°C (ASTM D648, 1.8 MPa, 3.2 mm thickness)
Flame Characteristics
Flammability: UL94 Class (at 3.2 mm thickness)
Injection Molding
- Pre-drying Conditions: 80–85°C for 3 hours
- Injection Pressure: 60–100 MPa
- Injection Speed: 50–80 mm/s
- Mold Temperature: 80°C
- Processing Temperature Range: Maximum 260°C
- Melt Temperature: 240°C
- Cylinder Temperature:
- Feeding: 220–240°C
- Compressing: 225–245°C
- Nozzle: 230–250°C
Features & Benefits
Optimized Processing Efficiency
With an MFR of 21 g/10min (260°C/5kg) and wide barrel temperatures (220°C–250°C), Suke D570 ensures fast, stable molding cycles—reducing energy use and production downtime.
Toughness Meets Rigidity
High impact strength (42 KJ/m² IZOD notched) and flexural modulus (1900 MPa) prevent cracks in drops/vibrations while maintaining dimensional stability for precision parts.
Reliable Thermal Performance
It resists deformation up to 86°C (1.8MPa HDT), ideal for components near heat sources (e.g., printer housings, power tools).
Use & Applications
- Electrical & Electronics: Power tool housings, router casings, connector components.
- Office Supplies: Printer/scanner panels, keyboard frames, durable desk accessories.