Suke FR865C GL ABS Resin Flame Retardant Grade

Suke FR865C GL is an eco-compliant, flame-retardant ABS resin engineered for high-flow applications. With UL94 V0 certification and RoHS compliance, it delivers exceptional safety and fluidity (40 g/10min MFR), ideal for precision components in electronics, printers, and office equipment.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Density: 1.17 g/cm³ (ASTM D792, 23°C)
Mechanical Properties
  • Tensile Strength: 40 MPa (ASTM D638, 50mm/min)
  • Flexural Strength: 67 MPa (ASTM D790, 2mm/min)
  • Flexural Modulus: 2100 MPa (ASTM D790, 2mm/min)
Impact Properties
  • Impact Strength (Izod Notched): 16 KJ/m² (ASTM D256, 3.2mm, 23°C)
Thermal Properties
  • Heat Distortion Temperature: 82°C (ASTM D648, 0.45 MPa, 6.4mm)
Flame Characteristics
  • Flammability: UL 94 V-0 (2.5mm)
Injection Molding
  • Pre-drying Condition: 80°C, 3 hours
  • Injection Pressure: 60-100 MPa
  • Injection Speed: 50-80 (unit unspecified)
  • Mold Temperature: 70°C
  • Processing Temperature Maximum: 230°C

Features & Benefits

Flame Safety Guaranteed

UL94 V0-rated at 2.5mm thickness, Suke FR865C GL eliminates fire risks in electronics and printers. No redesign needed for flame compliance.

Eco-Compliance Simplified

Passes RoHS standards effortlessly, ensuring global market access for eco-sensitive industries like office supplies and consumer electronics.

Precision Flow Mastery

High fluidity (40 g/10min MFR) enables thin-wall molding and intricate designs, reducing cycle times and production costs.

suke fr865c gl abs resin

Use & Applications

  • Printers: Fire-safe housings, gears, and structural parts.
  • Electrical & Electronics: Connectors, switches, and enclosures requiring V0 compliance.
  • Office Supplies: Durable, flame-retardant components for staplers, organizers, and device casings.