Suke Plastics FR965C ABS

suke plastics resin raw material granules 25kg package

Suke FR965C ABS Resin Flame Retardant Grade

Suke FR965C is a high-performance ABS resin engineered with TBBPA-based flame retardancy, achieving UL94 V-0 compliance at just 2.0mm thickness. Ideal for electronics and office equipment, it combines rigorous safety standards with reliable processability for high-volume manufacturing.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Density: 1.19 g/cm³ (ASTM D792, 23°C)
  • Mold Shrinkage: 0.4–0.7% (Internal Standard, 2 mm)
Mechanical Properties
  • Tensile Strength: 40 MPa (ASTM D638, 50 mm/min)
  • Elongation at Break: 10% (ASTM D638, 50 mm/min)
  • Flexural Strength: 68 MPa (ASTM D790, 2 mm/min)
  • Flexural Modulus: 2100 MPa (ASTM D790, 2 mm/min)
Impact Properties

Impact Strength (Izod Notched): 21 kJ/m² (ASTM D256, 3.2 mm, 23°C)

Thermal Properties
  • Heat Distortion Temperature: 77°C (ASTM D648, 0.45 MPa, 6.4 mm)
Flame Characteristics

Flammability: UL94 V-0 (2.0 mm thickness)

Injection Molding
  • Pre-drying Condition: 80°C for 3 hours
  • Injection Pressure: 60–100 MPa
  • Injection Speed: 50–80 mm/s
  • Mold Temperature: 70°C
  • Processing Temperature Range:
    • Melt Temperature: 200°C
    • Cylinder Temperature (Feeding): 170–190°C
    • Cylinder Temperature (Compressing): 180–200°C
    • Cylinder Temperature (Nozzle): 180–200°C

Features & Benefits

Guaranteed Fire Safety

It meets UL94 V-0 flammability standards (2.0mm), significantly reducing fire risks in electronics. Essential for compliance-sensitive applications like power strips and server housings.

Optimized Production Efficiency

High melt flow rate (50 g/10min @220°C) ensures fast injection molding with minimal energy. Pre-dries in 3 hours at 80°C, cutting downtime for urgent orders.

Balanced Mechanical Strength

It retains 40 MPa tensile strength and 21 kJ/m² impact resistance despite flame-retardant additives. Prevents brittle failures in thin-walled components like laptop casings.

suke fr965c abs resin

Use & Applications

  • Electronics & Electrical: Circuit breakers, connectors, power tool housings.
  • Office Supplies: Printer components, scanner frames, ergonomic device casings.
suke fr965c abs plastic application