Suke Plastics BC-173 SAN Resin

suke plastics resin raw material granules 25kg package

Suke BC-173 General Purpose Grade AS Resin

Suke BC-173 is a versatile SAN plastic resin designed for general molding applications. With superior mechanical performance and thermal stability, it’s perfect for industries requiring high precision, durability, and aesthetic quality in their parts.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Melt Flow Index: 13 g/10min (ASTM D1238, 220℃, 10kg)
Mechanical Properties
  • Flexural Strength: 110 MPa (ASTM D790, 2mm/min)
  • Flexural Modulus: 3700 MPa (ASTM D790, 2mm/min)
Impact Properties
  • Notched Izod Impact Strength: 20 J/m (ASTM D256, 23℃, 3.2mm)
Thermal Properties
  • Vicat Softening Temperature: 106℃ (ASTM D1525, 50N, 50℃/hr)
Injection Molding
  • Drying Temperature: 80-90℃
  • Drying Time: 2-4 Hours
  • Moisture Content: 0.01%
  • Melt Temperature: 190-210℃

Features & Benefits

Exceptional Mechanical Strength

Suke BC-173 features excellent flexural strength of 110 MPa and a flexural modulus of 3700 MPa (ASTM D790). This ensures durability and structural stability, even in demanding applications like lighter casings and small appliance components.

Reliable Thermal Performance

With a Vicat softening temperature of 106°C (ASTM D1525), Suke BC-173 delivers outstanding heat resistance, making it ideal for products exposed to moderate heat environments without compromising form or function.

Streamlined Processing Capabilities

The optimal melt flow index (13 g/10min) contributes to easy molding, ensuring precise shapes and consistent quality. It reduces production time while supporting intricate part designs for mass production requirements.

suke plastics resin raw material granules 25kg package

Use & Applications

  • Lighters and Small Appliances
  • Household Items and Consumer Goods
  • Industrial Components
suke plastics resin raw material granules 25kg package