Typical property data
Physical Properties
- Density: 1080 kg/m³ (ISO 1183, 23 °C)
- Melt Flow Rate (MFR): 18 g/10 min (ISO 1133, 220 °C / 10 kg)
- Mold Shrinkage: 0.4%−0.6% (ASTM D955, 23 °C / 50% RH)
Mechanical Properties
- Tensile Strength (Yield): 48MPa (ISO 527, 50 mm/min)
- Tensile Elongation at Break: 12% (ISO 527, 50 mm/min)
- Flexural Strength: 66MPa (ISO 178, 2 mm/min)
- Flexural Modulus: 1870MPa (ISO 178, 2 mm/min)
Impact Properties
- Charpy Notched Impact Strength: 12 kJ/m² (ISO 179/1eA, 23 °C / 50% RH)
Thermal Properties
- Deflection Temperature Under Load: 76°C (ISO 75, 1.8 MPa / 120 °C/hr)
Optical Properties
- Optical Properties: Light Transmittance: 86% (ASTM D1003, 3 mm thickness)
- Haze: 2% (ASTM D1003, 3 mm thickness)
Flame Characteristics
- Flammability Classification: HB (UL 94, File No. E41797)
Use & Applications
- E&E Products
- Household and Office Appliances
- Toys
Features & Benefits
1. High Optical Clarity
Designed for transparency, Toyolac™ 900 352 U achieves up to 86% light transmittance, delivering crystal-clear aesthetics for premium-looking products.
2. Balanced Strength and Flexibility
With a tensile strength of 48 MPa and 12% elongation at break, it provides exceptional durability while enabling complex product designs.
3. Consistent Dimensional Stability
Boasting a mold shrinkage of 0.4–0.6%, this material ensures precision in part dimensions, minimizing costly errors in production.