Toyolac™ 912 X01 U Transparent Grade Middle Impact Strength
Toyolac™ 912 X01 U is a transparent grade MABS plastic resin. It features the high scratch resistance, superior mechanical properties, excellent balance of clarity, toughness, and workability. Applications: E&E Products, Office Appliances, Toys.
Typical property data
Physical Properties
- Density: 1100 kg/m³ (ISO 1183, 23 °C)
- Melt Flow Rate: 30 g/10 min (ISO 1133, 220 °C / 10 kg)
Mechanical Properties
- Tensile Strength at Yield: 56 MPa (ISO 527, 50 mm/min)
- Tensile Elongation at Break: 10% (ISO 527, 50 mm/min)
- Flexural Strength: 83 MPa (ISO 178, 2 mm/min)
- Flexural Modulus: 2630 MPa (ISO 178, 2 mm/min)
Impact Properties
- Charpy Impact Strength, Notched: 6 kJ/m² (ISO 179/1eA, 23 °C / 50% RH)
Thermal Properties
- Deflection Temperature Under Load: 78 °C (ISO 75, 1.8 MPa / 120 °C/hr)
Optical Properties
- Light Transmittance: 78% (ASTM D1003, 3 mmt)
- Haze: 16% (ASTM D1003, 3 mmt)
Flame Characteristics
- Flammability: HB (UL 94, File No. E41797)
Use & Applications
- E&E Products
- Office Appliances
- Toys
Features & Benefits
1. High Scratch Resistance
Designed for durability, this resin resists surface damage, keeping products visually appealing and long-lasting in everyday use.
2. Excellent Transparency and Clarity
With 78% light transmittance, it ensures crystal-clear visuals, making it ideal for transparent electronic and appliance components.
3. Reliable Mechanical Strength
It offers 56 MPa tensile strength, delivering structural reliability for products requiring toughness in demanding environments.