TORAY Toyolac™ 990 X88

toray mabs resin 25kg package

Toyolac™ 990 X88 Transparent Grade Middle Impact Strength

Toyolac™ 990 X88 is a premium transparent MABS resin. It offers high impact strength, excellent flowability, exceptional optical clarity and versatile performance. Applications: E&E Products, Household and Office Appliances, Toys.

Associated Documents

ISO TDS - Data Sheet
UL Product iQ

Typical property data

Physical Properties
  • Density: 1090 kg/m³ (ISO 1183, 23 °C)
  • Melt Flow Rate: 26 g/10 min (ISO 1133, 220 °C / 10 kg)
  • Mold Shrinkage: 0.4%−0.6% (ASTM D955, 23 °C / 50% RH)
Mechanical Properties
  • Tensile Strength at Yield: 47 MPa (ISO 527, 50 mm/min)
  • Tensile Elongation at Break: 15% (ISO 527, 50 mm/min)
  • Tensile Modulus: 2250MPa (ISO 527, 1 mm/min)
  • Flexural Strength: 69 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2200 MPa (ISO 178, 2 mm/min)
Impact Properties
  • Charpy Impact Strength, Notched: 12 kJ/m² (ISO 179/1eA, 23 °C / 50% RH)
Thermal Properties
  • Deflection Temperature Under Load: 75 °C (ISO 75, 1.8 MPa / 120 °C/hr)
Optical Properties
  • Light Transmittance: 89% (ASTM D1003, 3 mmt)
  • Haze: 2% (ASTM D1003, 3 mm thickness)
Flame Characteristics
  • Flammability: Rating HB (UL 94 File No. E41797)

Use & Applications

  • E&E Products
  • Household and Office Appliances
  • Toys
toray mabs resin 25kg package

Features & Benefits

1. Exceptional Impact Strength

The high impact resistance of 12 kJ/m² ensures durability, reducing breakage risks in demanding environments.

2. Fast and Versatile Flow

With a 26 g/10 min Melt Flow Rate, it can achieve precision molding for both complex and thin designs.

3. Crystal-Clear Transparency

Featuring 89% light transmittance, it delivers superior optical clarity for visually appealing and functional end products.

toray mabs resin 25kg package

Send Us a Message