ULTEM™ Resin 1000P100

sabic ultem pei resin 25kg package

ULTEM™ Resin 1000P100 Unreinforced Amorphous PEI

ULTEM™ Resin 1000P100 is an unreinforced amorphous PEI powder with 100 µm D50 particle size. It offers 217°C Tg, 110 MPa tensile yield stress, and 47% LOI. It supports sintering, powder coating, and composite impregnation for high-heat, flame-retardant applications.

Associated Documents

TDS - Global

Typical property data

Physical Properties
  • Average Particle Size, D50: 100 micron
  • Maximum Particle Size, D100: 150 micron
  • Base Color: Transparent amber
  • Density: 1.27 g/cm³ (ISO 1183)
  • Specific Gravity: 1.27 (ASTM D792)
  • Moisture Absorption, 23°C / 50% RH / 24 hrs: 0.2% (ISO 62-4)
  • Moisture Absorption, 23°C / 50% RH / Equilibrium: 0.7% (ISO 62-4)
  • Water Absorption, 23°C / 24 hrs: 0.25% (ISO 62-1)
  • Water Absorption, 23°C / Saturated: 1.25% (ISO 62-1)
  • Water Absorption, 23°C / 24 hrs: 0.25% (ASTM D570)
  • Water Absorption, 23°C / Saturated: 1.25% (ASTM D570)
  • Melt Volume Rate, 360°C / 5.0 kg: 13 cm³/10 min (ISO 1133)
  • Melt Flow Rate, 337°C / 6.6 kgf: 9 g/10 min (ASTM D1238)
  • Poisson’s Ratio: 0.36 (ASTM E132)
Mechanical Properties
  • Tensile Stress, Yield, 50 mm/min: 110 MPa (ISO 527)
  • Tensile Strain, Yield, 50 mm/min: 6% (ISO 527)
  • Tensile Strain, Break, 50 mm/min: 50% (ISO 527)
  • Tensile Modulus, 1 mm/min: 3200 MPa (ISO 527)
  • Flexural Stress, Yield, 2 mm/min: 160 MPa (ISO 178)
  • Flexural Modulus, 2 mm/min: 3300 MPa (ISO 178)
  • Ball Indentation Hardness, H358/30: 140 MPa (ISO 2039-1)
  • Hardness, Rockwell M: 106 (ISO 2039-2)
  • Tensile Stress, Yield, Type I, 50 mm/min: 115 MPa (ASTM D638)
  • Tensile Strain, Yield, Type I, 50 mm/min: 7% (ASTM D638)
  • Tensile Strain, Break, Type I, 50 mm/min: 60% (ASTM D638)
  • Tensile Stress, Yield, Type I, 5 mm/min: 110 MPa (ASTM D638)
  • Tensile Strain, Yield, Type I, 5 mm/min: 7% (ASTM D638)
  • Tensile Strain, Break, Type I, 5 mm/min: 60% (ASTM D638)
  • Tensile Modulus, 5 mm/min: 3350 MPa (ASTM D638)
  • Flexural Stress, Yield, 1.3 mm/min, 50 mm Span: 165 MPa (ASTM D790)
  • Flexural Modulus, 1.3 mm/min, 50 mm Span: 3200 MPa (ASTM D790)
  • Flexural Stress, Yield, 2.6 mm/min, 100 mm Span: 160 MPa (ASTM D790)
  • Flexural Modulus, 2.6 mm/min, 100 mm Span: 3400 MPa (ASTM D790)
  • Hardness, Rockwell M: 109 (ASTM D785)
  • Taber Abrasion, CS-17, 1 kg: 10 mg/1000 cycles (ASTM D1044)
Impact Properties
  • Izod Impact, Unnotched, 80 × 10 × 4 mm, +23°C: NB (ISO 180/1U)
  • Izod Impact, Unnotched, 80 × 10 × 4 mm, -30°C: NB (ISO 180/1U)
  • Izod Impact, Unnotched, 23°C: 1800 J/m (ASTM D4812)
  • Izod Impact, Unnotched, -30°C: 1540 J/m (ASTM D4812)
  • Izod Impact, Notched, 80 × 10 × 4 mm, +23°C: 6 kJ/m² (ISO 180/1A)
  • Izod Impact, Notched, 80 × 10 × 4 mm, -30°C: 6 kJ/m² (ISO 180/1A)
  • Izod Impact, Notched, 23°C: 53 J/m (ASTM D256)
  • Izod Impact, Notched, -30°C: 50 J/m (ASTM D256)
  • Charpy Impact, V-Notch Edgewise, 80 × 10 × 4 mm, 23°C: 4 kJ/m² (ISO 179/1eA)
  • Charpy Impact, V-Notch Edgewise, 80 × 10 × 4 mm, -30°C: 4 kJ/m² (ISO 179/1eA)
  • Izod Impact, Reverse Notched, 3.2 mm: 1335 J/m (ASTM D256)
  • Gardner Impact, 23°C: 36 J (ASTM D3029)
Thermal Properties
  • Glass Transition Temperature, Tg: 217°C
  • HDT/Bf, 0.45 MPa, Flatwise, 80 × 10 × 4 mm: 209°C (ISO 75/Bf)
  • HDT/Af, 1.8 MPa, Flatwise, 80 × 10 × 4 mm: 192°C (ISO 75/Af)
  • HDT, 0.45 MPa, 6.4 mm, Unannealed: 210°C (ASTM D648)
  • HDT, 1.82 MPa, 6.4 mm, Unannealed: 201°C (ASTM D648)
  • HDT, 0.45 MPa, 3.2 mm, Unannealed: 207°C (ASTM D648)
  • HDT, 1.82 MPa, 3.2 mm, Unannealed: 190°C (ASTM D648)
  • Vicat Softening Temperature, Rate A/50: 215°C (ISO 306)
  • Vicat Softening Temperature, Rate B/50: 211°C (ISO 306)
  • Vicat Softening Temperature, Rate B/120: 212°C (ISO 306)
  • Vicat Softening Temperature, Rate B/50: 211°C (ASTM D1525)
  • CTE, -40°C to 150°C, Flow: 5.2E-05 1/°C (ISO 11359-2)
  • CTE, -40°C to 150°C, X-Flow: 5.2E-05 1/°C (ISO 11359-2)
  • CTE, -20°C to 150°C, Flow: 5.6E-05 1/°C (ASTM E831)
  • CTE, -20°C to 150°C, X-Flow: 5.4E-05 1/°C (ASTM E831)
  • Thermal Conductivity: 0.22 W/m·°C (ISO 8302)
  • Thermal Conductivity: 0.22 W/m·°C (ASTM C177)
  • Ball Pressure Test, 125°C ± 2°C: PASS (IEC 60695-10-2)
Electrical Properties
  • Volume Resistivity: 1.0E+15 Ω·cm (IEC 60093)
  • Surface Resistivity, ROA: >1.0E+15 Ω (IEC 60093)
  • Volume Resistivity: 1.0E+17 Ω·cm (ASTM D257)
  • Dielectric Strength, In Oil, 0.8 mm: 33 kV/mm (IEC 60243-1)
  • Dielectric Strength, In Oil, 1.6 mm: 25 kV/mm (IEC 60243-1)
  • Dielectric Strength, In Oil, 3.2 mm: 16 kV/mm (IEC 60243-1)
  • Dielectric Strength, In Air, 1.6 mm: 32.7 kV/mm (ASTM D149)
  • Dielectric Strength, In Oil, 1.6 mm: 28.0 kV/mm (ASTM D149)
  • Dielectric Strength, In Oil, 3.2 mm: 19.7 kV/mm (ASTM D149)
  • Relative Permittivity, 1 MHz: 2.9 (IEC 60250)
  • Relative Permittivity, 50/60 Hz: 2.9 (IEC 60250)
  • Relative Permittivity, 100 Hz: 3.15 (ASTM D150)
  • Relative Permittivity, 1 kHz: 3.15 (ASTM D150)
  • Dielectric Constant, 1.1 GHz: 3.01
  • Dielectric Constant, 5 GHz: 3.02
  • Dielectric Constant, 10 GHz: 3.02
  • Dissipation Factor, 1.1 GHz: 0.0012
  • Dissipation Factor, 5 GHz: 0.0024
  • Dissipation Factor, 10 GHz: 0.0027
  • Comparative Tracking Index: 150 V (IEC 60112)
  • Comparative Tracking Index, M: 100 V (IEC 60112)
Flame Characteristics
  • Oxygen Index LOI: 47% ASTM D2863
  • Oxygen Index LOI: 47% ISO 4589
  • Flame Retardancy: Inherently flame retardant
  • Flame Retardant System: Non-halogenated flame retardant
  • Smoke / Toxicity Feature: Low smoke and toxicity
Processing Parameters
  • Processing Techniques: Sintering, Powder Coating, Impregnation for composites
  • Material Form: Powder
  • Average Particle Size, D50: 100 micron
  • Maximum Particle Size, D100: 150 micron
  • Melt Volume Rate, 360°C / 5.0 kg: 13 cm³/10 min (ISO 1133)
  • Melt Flow Rate, 337°C / 6.6 kgf: 9 g/10 min (ASTM D1238)
  • Filler: Unreinforced
  • Morphology: Amorphous

Use & Applications

  • Automotive
  • building & construction
  • consumer
  • E&E
  • industrial
  • mass transportation
  • packaging
sabic ultem pei resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.