ULTEM™ Resin 1010TC

sabic ultem pei resin 25kg package

ULTEM™ Resin 1010TC

ULTEM™ Resin 1010TC is an unreinforced PEI resin with high flow and a 217°C Tg. It offers strong mechanical, electrical, and dimensional performance at high temperatures. Inherent UL94 V-0 and 5VA flame ratings, low smoke, IR transparency, and RoHS compliance support demanding electronic and consumer parts.

Associated Documents

TDS - Global

Typical property data

Physical Properties
  • Density: 1.27 g/cm³ (ISO 1183)
  • Specific Gravity: 1.27 (ASTM D792)
  • Moisture Absorption, 23°C / 50% RH / 24 hrs: 0.2% (ISO 62-4)
  • Moisture Absorption, 23°C / 50% RH / Equilibrium: 0.7% (ISO 62-4)
  • Water Absorption, 23°C / 24 hrs: 0.25% (ISO 62-1)
  • Water Absorption, 23°C / Saturated: 1.25% (ISO 62-1)
  • Water Absorption, 23°C / 24 hrs: 0.25% (ASTM D570)
  • Water Absorption, 23°C / Saturated: 1.25% (ASTM D570)
  • Melt Volume Rate, 360°C / 5.0 kg: 25 cm³/10 min (ISO 1133)
  • Melt Volume Rate, 340°C / 5.0 kg: 13 cm³/10 min (ISO 1133)
  • Melt Flow Rate, 337°C / 6.6 kgf: 17.8 g/10 min (ASTM D1238)
  • Poisson’s Ratio: 0.36 (ASTM E132)
  • Mold Shrinkage, Flow, 3.2 mm: 0.5–0.7% (SABIC Method)
  • Mold Shrinkage, Cross Flow, 3.2 mm: 0.5–0.7% (SABIC Method)
Mechanical Properties
  • Tensile Stress at Yield, 50 mm/min: 110 MPa (ISO 527)
  • Tensile Strain at Yield, 50 mm/min: 6% (ISO 527)
  • Tensile Strain at Break, 50 mm/min: 50% (ISO 527)
  • Tensile Modulus, 1 mm/min: 3200 MPa (ISO 527)
  • Flexural Stress at Yield, 2 mm/min: 160 MPa (ISO 178)
  • Flexural Modulus, 2 mm/min: 3300 MPa (ISO 178)
  • Ball Indentation Hardness, H358/30: 140 MPa (ISO 2039-1)
  • Rockwell Hardness, M Scale: 106 (ISO 2039-2)
  • Tensile Stress at Yield, Type I, 50 mm/min: 115 MPa (ASTM D638)
  • Tensile Strain at Yield, Type I, 50 mm/min: 7% (ASTM D638)
  • Tensile Strain at Break, Type I, 50 mm/min: 60% (ASTM D638)
  • Tensile Stress at Yield, Type I, 5 mm/min: 110 MPa (ASTM D638)
  • Tensile Modulus, 5 mm/min: 3350 MPa (ASTM D638)
  • Flexural Stress at Yield, 1.3 mm/min, 50 mm Span: 165 MPa (ASTM D790)
  • Flexural Modulus, 1.3 mm/min, 50 mm Span: 3200 MPa (ASTM D790)
  • Flexural Stress at Yield, 2.6 mm/min, 100 mm Span: 160 MPa (ASTM D790)
  • Flexural Modulus, 2.6 mm/min, 100 mm Span: 3400 MPa (ASTM D790)
  • Rockwell Hardness, M Scale: 109 (ASTM D785)
  • Taber Abrasion, CS-17, 1 kg: 10 mg/1000 cycles (ASTM D1044)
Impact Properties
  • Izod Impact, Unnotched, 80 × 10 × 4 mm, +23°C: NB (ISO 180/1U)
  • Izod Impact, Unnotched, 80 × 10 × 4 mm, -30°C: NB (ISO 180/1U)
  • Izod Impact, Unnotched, 23°C: 1600 J/m (ASTM D4812)
  • Izod Impact, Unnotched, -30°C: 1500 J/m (ASTM D4812)
  • Izod Impact, Notched, 80 × 10 × 4 mm, +23°C: 5 kJ/m² (ISO 180/1A)
  • Izod Impact, Notched, 80 × 10 × 4 mm, -30°C: 5 kJ/m² (ISO 180/1A)
  • Izod Impact, Notched, 23°C: 32 J/m (ASTM D256)
  • Izod Impact, Notched, -30°C: 41 J/m (ASTM D256)
  • Charpy Impact, V-Notch Edgewise, 23°C: 4 kJ/m² (ISO 179/1eA)
  • Charpy Impact, V-Notch Edgewise, -30°C: 4 kJ/m² (ISO 179/1eA)
  • Izod Impact, Reverse Notched, 3.2 mm: 1174 J/m (ASTM D256)
  • Gardner Impact, 23°C: 33 J (SABIC Method)
Thermal Properties
  • Glass Transition Temperature, Tg: 217°C
  • Heat Deflection Temperature, 0.45 MPa, Flatwise: 209°C (ISO 75/Bf)
  • Heat Deflection Temperature, 1.8 MPa, Flatwise: 192°C (ISO 75/Af)
  • Heat Deflection Temperature, 0.45 MPa, 6.4 mm, Unannealed: 210°C (ASTM D648)
  • Heat Deflection Temperature, 1.82 MPa, 6.4 mm, Unannealed: 201°C (ASTM D648)
  • Heat Deflection Temperature, 0.45 MPa, 3.2 mm, Unannealed: 207°C (ASTM D648)
  • Heat Deflection Temperature, 1.82 MPa, 3.2 mm, Unannealed: 190°C (ASTM D648)
  • Vicat Softening Temperature, Rate A/50: 215°C (ISO 306)
  • Vicat Softening Temperature, Rate B/50: 211°C (ISO 306)
  • Vicat Softening Temperature, Rate B/120: 212°C (ISO 306)
  • Vicat Softening Temperature, Rate B/50: 211°C (ASTM D1525)
  • Coefficient of Thermal Expansion, -40°C to 150°C, Flow: 5.2E-05 1/°C (ISO 11359-2)
  • Coefficient of Thermal Expansion, -40°C to 150°C, Cross Flow: 5.2E-05 1/°C (ISO 11359-2)
  • Coefficient of Thermal Expansion, -20°C to 150°C, Flow: 5.2E-05 1/°C (ASTM E831)
  • Coefficient of Thermal Expansion, -20°C to 150°C, Cross Flow: 5.2E-05 1/°C (ASTM E831)
  • Ball Pressure Test, 125°C ± 2°C: PASS (IEC 60695-10-2)
  • Thermal Conductivity: 0.22 W/m·°C (ISO 8302)
  • Thermal Conductivity: 0.22 W/m·°C (ASTM C177)
  • Relative Temperature Index, Electrical: 170°C (UL 746B)
  • Relative Temperature Index, Mechanical with Impact: 170°C (UL 746B)
  • Relative Temperature Index, Mechanical without Impact: 170°C (UL 746B)
Optical Properties
  • Light Transmission: Controlled light transmission levels by color
  • Transparency: Transparent / Translucent grade
Electrical Properties
  • Volume Resistivity: 1.0E+15 Ω·cm (IEC 60093)
  • Surface Resistivity, ROA: >1.0E+15 Ω (IEC 60093)
  • Volume Resistivity: 1.0E+17 Ω·cm (ASTM D257)
  • Dielectric Strength, in Oil, 0.8 mm: 33 kV/mm (IEC 60243-1)
  • Dielectric Strength, in Oil, 1.6 mm: 25 kV/mm (IEC 60243-1)
  • Dielectric Strength, in Oil, 3.2 mm: 16 kV/mm (IEC 60243-1)
  • Dielectric Strength, in Air, 1.6 mm: 32.7 kV/mm (ASTM D149)
  • Dielectric Strength, in Oil, 1.6 mm: 28.0 kV/mm (ASTM D149)
  • Dielectric Strength, in Oil, 3.2 mm: 19.7 kV/mm (ASTM D149)
  • Relative Permittivity, 1 MHz: 2.9 (IEC 60250)
  • Relative Permittivity, 50/60 Hz: 2.9 (IEC 60250)
  • Relative Permittivity, 100 Hz: 3.15 (ASTM D150)
  • Relative Permittivity, 1 kHz: 3.15 (ASTM D150)
  • Dielectric Constant, 1.1 GHz: 3.01
  • Dielectric Constant, 5 GHz: 3.02
  • Dielectric Constant, 10 GHz: 3.02
  • Dissipation Factor, 1.1 GHz: 0.0012
  • Dissipation Factor, 5 GHz: 0.0024
  • Dissipation Factor, 10 GHz: 0.0027
  • Comparative Tracking Index: 150 V (IEC 60112)
  • Comparative Tracking Index, M: 100 V (IEC 60112)
  • Comparative Tracking Index, UL PLC: 4 PLC Code (UL 746A)
  • Hot-Wire Ignition, PLC 1: ≥3 mm (UL 746A)
  • Hot-Wire Ignition, PLC 2: ≥1.5 mm (UL 746A)
  • High Amp Arc Ignition, PLC 3: ≥3 mm (UL 746A)
  • High Amp Arc Ignition, PLC 4: ≥1.5 mm (UL 746A)
  • High Voltage Arc Track Rate, PLC: 4 PLC Code (UL 746A)
  • Arc Resistance, Tungsten, PLC: 5 PLC Code (ASTM D495)
Flame Characteristics
  • UL 94 5VA Flame Class Rating: ≥3 mm (UL 94)
  • UL 94 V-0 Flame Class Rating: ≥1.5 mm (UL 94)
  • Oxygen Index, LOI: 44% (ASTM D2863)
  • Oxygen Index, LOI: 47% (ISO 4589)
  • NBS Smoke Density, Flaming, Ds 4 min: 2 (ASTM E662)
  • Flame Retardant System: Non-halogenated flame retardant
  • Flame Retardancy: Inherently flame retardant
Injection Molding Processing
  • Drying Temperature: 150°C
  • Drying Time: 4–6 hrs
  • Cumulative Drying Time: 24 hrs
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 350–410°C
  • Nozzle Temperature: 345–405°C
  • Front Zone 3 Temperature: 345–415°C
  • Middle Zone 2 Temperature: 340–405°C
  • Rear Zone 1 Temperature: 330–400°C
  • Mold Temperature: 135–180°C
  • Back Pressure: 0.3–0.7 MPa
  • Screw Speed, Circumferential Speed: 0.2–0.3 m/s
  • Shot to Cylinder Size: 40–60%
  • Vent Depth: 0.025–0.076 mm
Extrusion Blow Molding Processing
  • Drying Temperature: 140–150°C
  • Drying Time: 4–6 hrs
  • Cumulative Drying Time: 24 hrs
  • Maximum Moisture Content: 0.01–0.02%
  • Melt Temperature, Parison: 320–355°C
  • Barrel Zone 1 Temperature: 325–350°C
  • Barrel Zone 2 Temperature: 330–355°C
  • Barrel Zone 3 Temperature: 330–355°C
  • Barrel Zone 4 Temperature: 330–355°C
  • Adapter Zone 5 Temperature: 330–355°C
  • Head Zone 6 Top Temperature: 330–355°C
  • Head Zone 7 Bottom Temperature: 330–355°C
  • Screw Speed: 10–70 rpm
  • Mold Temperature: 65–175°C
  • Die Temperature: 325–355°C

Use & Applications

  • Consumer
  • E&E
sabic ultem pei resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.