ULTEM™ Resin 1110F

sabic ultem pei resin 25kg package

ULTEM™ Resin 1110F

ULTEM™ Resin 1110F is an enhanced-flow PEI resin for injection molding. It delivers 217°C Tg, 198°C HDT, UL94 V-0 at 0.75 mm, and 110 MPa tensile yield strength. It supports thin-wall parts needing heat resistance, flame safety, low warpage, and stable dimensions.

Associated Documents

TDS - Asia
TDS - Americas
TDS - Europe

Typical property data

Physical Properties
  • Specific Gravity: 1.36 (ASTM D792)
  • Mold Shrinkage, Flow, 3.2 mm: 0.5–0.7% (SABIC Method)
  • Melt Flow Rate, 337°C/6.6 kgf: 16 g/10 min (ASTM D1238)
Mechanical Properties
  • Tensile Stress at Yield, Type I, 5 mm/min: 110 MPa (ASTM D638)
  • Tensile Strain at Break, Type I, 5 mm/min: 70% (ASTM D638)
  • Tensile Modulus, 5 mm/min: 3720 MPa (ASTM D638)
  • Flexural Stress at Yield, 2.6 mm/min, 100 mm Span: 165 MPa (ASTM D790)
  • Flexural Modulus, 2.6 mm/min, 100 mm Span: 3720 MPa (ASTM D790)
  • Izod Impact, Reverse Notched, 3.2 mm: 1922 J/m (ASTM D256)
  • Gardner Impact, 23°C: 23 J (ASTM D3029)
Thermal Properties
  • Glass Transition Temperature, Tg: 217°C (SABIC Datasheet Description)
  • Heat Deflection Temperature, 1.82 MPa, 6.4 mm, Unannealed: 198°C (ASTM D648)
  • Relative Temperature Index, Electrical: 170°C (UL 746B)
  • Relative Temperature Index, Mechanical with Impact: 170°C (UL 746B)
  • Relative Temperature Index, Mechanical without Impact: 170°C (UL 746B)
Electrical Properties
  • Arc Resistance, Tungsten: PLC 5 (ASTM D495)
  • High Voltage Arc Tracking Rate: PLC 2 (UL 746A)
  • Comparative Tracking Index, UL: PLC 4 (UL 746A)
  • Hot-Wire Ignition, PLC 1: ≥3 mm (UL 746A)
  • Hot-Wire Ignition, PLC 2: ≥0.75 mm (UL 746A)
  • High Amp Arc Ignition, PLC 3: ≥3 mm (UL 746A)
  • High Amp Arc Ignition, PLC 4: ≥0.75 mm (UL 746A)
Flame Characteristics
  • UL Recognized 94-5VA Flame Class Rating: ≥3 mm (UL 94)
  • UL Recognized 94V-0 Flame Class Rating: ≥0.75 mm (UL 94)
  • UL Recognized 94V-2 Flame Class Rating: ≥0.4 mm (UL 94)
  • Flame Retardant System: Non-halogenated flame retardant
  • Low Smoke and Toxicity: Listed feature in datasheet
Injection Molding Processing
  • Drying Temperature: 150°C
  • Drying Time: 4–6 hrs
  • Cumulative Drying Time: 24 hrs
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 350–400°C
  • Nozzle Temperature: 345–400°C
  • Front Zone 3 Temperature: 345–400°C
  • Middle Zone 2 Temperature: 340–400°C
  • Rear Zone 1 Temperature: 330–400°C
  • Mold Temperature: 135–165°C
  • Back Pressure: 0.3–0.7 MPa
  • Screw Speed: 40–70 rpm
  • Shot to Cylinder Size: 40–60%
  • Vent Depth: 0.025–0.076 mm

Use & Applications

  • Automotive
  • building & construction
  • consumer
  • E&E
  • healthcare
  • industrial
  • mass transportation
  • packaging
sabic ultem pei resin 25kg package