Plastic Granules
ULTEM™ Resin 2310R 30% Glass Fiber Reinforced Polyetherimide (PEI)
ULTEM™ Resin 2310R is a 30% glass fiber reinforced PEI with improved flow and internal mold release. It offers high stiffness, low shrinkage, heat resistance up to 210°C HDT, and UL 94 V-0 flame performance for precision molded parts.
Associated Documents
TDS - Global Data Sheet
Typical property data
Physical Properties
- Density: 1.51 g/cm³ (ISO 1183)
- Specific Gravity: 1.51 (ASTM D792)
- Moisture Absorption, 23°C / 50% RH / 24 hrs: 0.1% (ISO 62-4)
- Moisture Absorption, 23°C / 50% RH / Equilibrium: 0.6% (ISO 62-4)
- Water Absorption, 23°C / 24 hrs: 0.16% (ISO 62-1)
- Water Absorption, 23°C / Saturated: 0.9% (ISO 62-1)
- Water Absorption, 23°C / 24 hrs: 0.16% (ASTM D570)
- Water Absorption, 23°C / Saturated: 0.9% (ASTM D570)
- Mold Shrinkage, Flow, 3.2 mm: 0.2–0.4% (SABIC Method)
Mechanical Properties
- Tensile Stress at Break, 5 mm/min: 175 MPa (ISO 527)
- Tensile Strain at Break, 5 mm/min: 2.4% (ISO 527)
- Tensile Modulus, 1 mm/min: 10,500 MPa (ISO 527)
- Flexural Stress at Break, 2 mm/min: 240 MPa (ISO 178)
- Flexural Modulus, 2 mm/min: 9,600 MPa (ISO 178)
- Ball Indentation Hardness, H358/30: 165 MPa (ISO 2039-1)
- Taber Abrasion, CS-17, 1 kg: 20 mg/1000 cycles (SABIC Method)
- Rockwell Hardness: M110 (ISO 2039-2)
- Tensile Stress at Break, Type I, 5 mm/min: 175 MPa (ASTM D638)
- Tensile Strain at Break, Type I, 5 mm/min: 2.5% (ASTM D638)
- Tensile Modulus, 5 mm/min: 10,400 MPa (ASTM D638)
- Flexural Stress at Break, 2.6 mm/min, 100 mm span: 230 MPa (ASTM D790)
- Flexural Modulus, 2.6 mm/min, 100 mm span: 9,400 MPa (ASTM D790)
- Flexural Stress at Break, 1.3 mm/min, 50 mm span: 250 MPa (ASTM D790)
- Flexural Modulus, 1.3 mm/min, 50 mm span: 9,700 MPa (ASTM D790)
- Rockwell Hardness: M114 (ASTM D785)
Impact Properties
- Notched Izod Impact, 80 × 10 × 4 mm, +23°C: 10 kJ/m² (ISO 180/1A)
- Notched Izod Impact, 80 × 10 × 4 mm, -30°C: 10 kJ/m² (ISO 180/1A)
- Notched Izod Impact, 23°C: 90 J/m (ASTM D256)
- Notched Izod Impact, -30°C: 80 J/m (ASTM D256)
- Unnotched Izod Impact, 80 × 10 × 4 mm, +23°C: 40 kJ/m² (ISO 180/1U)
- Unnotched Izod Impact, 80 × 10 × 4 mm, -30°C: 40 kJ/m² (ISO 180/1U)
- Unnotched Izod Impact, 23°C: 600 J/m (ASTM D4812)
- Unnotched Izod Impact, -30°C: 600 J/m (ASTM D4812)
- Charpy Impact, V-Notch Edgewise, 23°C: 10 kJ/m² (ISO 179/1eA)
- Charpy Impact, V-Notch Edgewise, -30°C: 10 kJ/m² (ISO 179/1eA)
- Charpy Impact, Unnotched Edgewise, 23°C: 40 kJ/m² (ISO 179/1eU)
- Charpy Impact, Unnotched Edgewise, -30°C: 40 kJ/m² (ISO 179/1eU)
- Reverse Notched Izod Impact, 3.2 mm: 470 J/m (ASTM D256)
Thermal Properties
- Glass Transition Temperature: 217°C (from product description)
- HDT/Bf, 0.45 MPa, Flatwise, 80 × 10 × 4 mm: 215°C (ISO 75/Bf)
- HDT/Af, 1.8 MPa, Flatwise, 80 × 10 × 4 mm: 210°C (ISO 75/Af)
- Vicat Softening Temperature, Rate A/50: 225°C (ISO 306)
- Vicat Softening Temperature, Rate B/120: 220°C (ISO 306)
- Vicat Softening Temperature, Rate B/50: 213°C (ISO 306)
- CTE, -40°C to 150°C, Flow: 1.8E-05 1/°C (ISO 11359-2)
- CTE, -40°C to 150°C, Cross Flow: 4.8E-05 1/°C (ISO 11359-2)
- Thermal Conductivity: 0.31 W/m·°C (ISO 8302)
- Ball Pressure Test, 125°C ± 2°C: Pass (IEC 60695-10-2)
- HDT, 0.45 MPa, 3.2 mm, Unannealed: 215°C (ASTM D648)
- HDT, 0.45 MPa, 6.4 mm, Unannealed: 212°C (ASTM D648)
- HDT, 1.82 MPa, 3.2 mm, Unannealed: 211°C (ASTM D648)
- HDT, 1.82 MPa, 6.4 mm, Unannealed: 210°C (ASTM D648)
- CTE, -20°C to 150°C, Flow: 1.8E-05 1/°C (ASTM E831)
- CTE, -20°C to 150°C, Cross Flow: 4.8E-05 1/°C (ASTM E831)
- Relative Temperature Index, Electrical: 180°C (UL 746B)
- Relative Temperature Index, Mechanical with Impact: 170°C (UL 746B)
- Relative Temperature Index, Mechanical without Impact: 180°C (UL 746B)
Electrical Properties
- Volume Resistivity: 1.0E+15 Ω·cm (IEC 60093)
- Surface Resistivity, ROA: >1.0E+15 Ω (IEC 60093)
- Dielectric Strength, in Oil, 0.8 mm: 35 kV/mm (IEC 60243-1)
- Dielectric Strength, in Oil, 1.6 mm: 26 kV/mm (IEC 60243-1)
- Dielectric Strength, in Oil, 3.2 mm: 15 kV/mm (IEC 60243-1)
- Relative Permittivity, 50/60 Hz: 3.3 (IEC 60250)
- Relative Permittivity, 1 MHz: 3.4 (IEC 60250)
- Dielectric Constant, 1.1 GHz: 3.51 (Internal / SPDR dry as molded specimen)
- Dielectric Constant, 5 GHz: 3.59 (Internal / SPDR dry as molded specimen)
- Dielectric Constant, 10 GHz: 3.60 (Internal / SPDR dry as molded specimen)
- Dissipation Factor, 50/60 Hz: 0.0016 (IEC 60250)
- Dissipation Factor, 1 MHz: 0.0023 (IEC 60250)
- Dissipation Factor, 1.1 GHz: 0.0029 (Internal / SPDR dry as molded specimen)
- Dissipation Factor, 5 GHz: 0.0036 (Internal / SPDR dry as molded specimen)
- Dissipation Factor, 10 GHz: 0.0046 (Internal / SPDR dry as molded specimen)
- Dissipation Factor, 1 kHz: 0.0015 (ASTM D150)
- Comparative Tracking Index: 150 V (IEC 60112)
- Comparative Tracking Index, M: 100 V (IEC 60112)
- Volume Resistivity: 3.0E+16 Ω·cm (ASTM D257)
- Dielectric Strength, in Air, 1.6 mm: 24.8 kV/mm (ASTM D149)
- Dielectric Strength, in Oil, 1.6 mm: 30.3 kV/mm (ASTM D149)
- Relative Permittivity, 1 kHz: 3.7 (ASTM D150)
- Comparative Tracking Index, UL PLC: PLC 4 (UL 746A)
- Hot-Wire Ignition, PLC 1: ≥3 mm (UL 746A)
- Hot-Wire Ignition, PLC 3: ≥1.5 mm (UL 746A)
- High Amp Arc Ignition, PLC 3: ≥1.5 mm (UL 746A)
- High Amp Arc Ignition, PLC 4: ≥3 mm (UL 746A)
- High Voltage Arc Track Rate: PLC 3 (UL 746A)
- Arc Resistance, Tungsten: PLC 6 (ASTM D495)
Flame Characteristics
- UL Recognized 94-5VA Flame Class Rating: ≥1.2 mm (UL 94)
- UL Recognized 94V-0 Flame Class Rating: ≥0.25 mm (UL 94)
- Glow Wire Ignitability Temperature, 2.0 mm: 900°C (IEC 60695-2-13)
- Glow Wire Flammability Index, 2.0 mm: 960°C (IEC 60695-2-12)
- UV-Light / Water Exposure / Immersion: F1 (UL 746C)
- Oxygen Index, LOI: 48% (ISO 4589)
Processing Parameters
- Drying Temperature: 150°C
- Drying Time: 4–6 hrs
- Drying Time, Cumulative: 24 hrs
- Maximum Moisture Content: 0.02%
- Melt Temperature: 350–410°C
- Nozzle Temperature: 345–410°C
- Front Zone 3 Temperature: 345–420°C
- Middle Zone 2 Temperature: 340–410°C
- Rear Zone 1 Temperature: 330–400°C
- Hopper Temperature: 80–120°C
- Mold Temperature: 135–180°C
- Shot to Cylinder Size: 40–60%
- Vent Depth: 0.025–0.076 mm
- Screw Circumferential Speed: 0.15–0.25 m/s
- Screw Speed: 40–70 rpm
- Back Pressure: 0.3–1.5 MPa
Use & Applications
- for precision electrical, automotive, aerospace, industrial, and high-performance molded components.