VALOX™ FR Resin 553 is a 30% glass-filled, flame-retardant PBT/PC alloy. It offers excellent chemical resistance, superior dimensional stability with low warpage, and top-tier UL94 V-0 & 5VA flammability ratings for demanding applications.

Associated Documents

TDS Asia
TDS Americas
TDS Europe

Typical property data

Physical Properties

Density: 1.53 g/cm³ (ISO 1183)

Mechanical Properties
  • Tensile Strength: 55 MPa (ISO 527)
  • Tensile Modulus: 3600 MPa (ISO 527)
  • Flexural Strength: 90 MPa (ISO 178)
  • Flexural Modulus: 3600 MPa (ISO 178)
  • Elongation at Break: 2.5% (ISO 527)
Impact Properties
  • Charpy Notched Impact Strength (23°C): 8 kJ/m² (ISO 179/1eA)
  • Charpy Notched Impact Strength (-30°C): 6 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Glass Transition Temperature (Tg): N/A
  • Melting Temperature (Tm): 225°C (ISO 11357)
  • Heat Deflection Temperature (HDT, 1.8 MPa): 170°C (ISO 75-2/A)
  • Coefficient of Linear Thermal Expansion (CLTE): 0.3 x 10⁻⁴ /°C (ISO 11359)
Electrical Properties
  • Comparative Tracking Index (CTI): 600 V (IEC 60112)
  • Dielectric Strength: 20 kV/mm (IEC 60243-1)
  • Volume Resistivity: 1 x 10¹⁵ Ω·cm (IEC 60093)
  • Dielectric Constant (1 MHz): 3.4 (IEC 60250)
Flame Characteristics

Flammability Rating: UL94 V-0 (Thickness: 0.75 mm)

Injection Molding
  • Melt Temperature: 240–260°C
  • Mold Temperature: 80–120°C
  • Drying Temperature: 110°C
  • Drying Time: 4–6 hours

Features & Benefits

Superior Flame Retardant Performance

VALOX 553 achieves UL94 V-0 at 0.86mm and 5VA at 2.3mm, ensuring critical safety compliance and enhanced product integrity in electrical and electronic components.

Excellent Dimensional Stability

Its 30% glass-fiber reinforcement minimizes shrinkage and warpage, guaranteeing precise part geometry and long-term reliability in tightly toleranced assemblies.

High Heat & Chemical Resistance

With a Heat Deflection Temperature of 160°C and excellent chemical resistance, VALOX 553 withstands harsh operating environments and extends product service life.

30% glass filled valox fr pbt resin

Use & Application

  • Appliance Handles and Housings
  • Spotlights and Electrical Enclosures
  • Electric Motor Components
  • Pump Housings and Impellers
30% glass filled valox fr pbt resin

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.