Sabic VALOX™ FR PBT 855

sabic valox fr pbt

Valox FR PBT 855 Flame Retardant Grade

VALOX™ FR PBT 855 is a 15% glass-filled, flame-retardant PBT/PET compound. It offers a UL94 V-0 rating at 1.5mm, excellent chemical resistance, and superior aesthetics for demanding applications like appliances and lighting.

Associated Documents

TDS Asia
TDS Americas
TDS Europe

Typical property data

Physical Properties
  • Specific Gravity: 1.5 (ASTM D792)
  • Specific Volume: 0.65 cm³/g (ASTM D792)
  • Water Absorption (23°C/24 hrs): 0.06% (ASTM D570)
  • Mold Shrinkage (flow, 1.5-3.2 mm): 0.4 – 0.6% (SABIC method)
  • Mold Shrinkage (flow, 3.2-4.6 mm): 0.6 – 0.9% (SABIC method)
  • Mold Shrinkage (xflow, 1.5-3.2 mm): 0.5 – 0.8% (SABIC method)
  • Mold Shrinkage (xflow, 3.2-4.6 mm): 0.8 – 1.1% (SABIC method)
  • Melt Flow Rate (266°C/5.0 kgf): 79 g/10 min (ASTM D1238)
Mechanical Properties
  • Tensile Stress (break, Type I, 5 mm/min): 95 MPa (ASTM D638)
  • Flexural Stress (break, 1.3 mm/min, 50 mm span): 143 MPa (ASTM D790)
  • Flexural Modulus (1.3 mm/min, 50 mm span): 5000 MPa (ASTM D790)
  • Hardness (Rockwell R): 119 (ASTM D785)
Impact Properties
  • Izod Impact (unnotched, 23°C): 345 J/m (ASTM D4812)
  • Izod Impact (notched, 23°C): 55 J/m (ASTM D256)
Thermal Properties
  • HDT (0.45 MPa, 6.4 mm, unannealed): 204°C (ASTM D648)
  • HDT (1.82 MPa, 6.4 mm, unannealed): 187°C (ASTM D648)
  • CTE (-40°C to 40°C, flow): 4.0E-05 1/°C (ASTM E831)
  • CTE (60°C to 138°C, flow): 6.12E-05 1/°C (ASTM E831)
  • Relative Temp Index (Electrical): 125°C (UL 746B)
  • Relative Temp Index (Mechanical with impact): 110°C (UL 746B)
  • Relative Temp Index (Mechanical without impact): 125°C (UL 746B)
Electrical Properties
  • Volume Resistivity: 1.0E+13 Ω·cm (ASTM D257)
  • Dielectric Strength (in air, 3.2 mm): 20 kV/mm (ASTM D149)
  • Dielectric Strength (in oil, 1.6 mm): 24 kV/mm (ASTM D149)
  • Relative Permittivity (100 Hz): 3.5 (ASTM D150)
  • Relative Permittivity (1 MHz): 3.3 (ASTM D150)
  • Dissipation Factor (100 Hz): 0.001 (ASTM D150)
  • Dissipation Factor (1 MHz): 0.0125 (ASTM D150)
  • Arc Resistance (Tungsten): PLC Code 6 (ASTM D495)
  • Hot Wire Ignition: PLC Code 0 (UL 746A)
  • High Voltage Arc Track Rate: PLC Code 4 (UL 746A)
  • High Ampere Arc Ignition (surface): PLC Code 4 (UL 746A)
  • Comparative Tracking Index (UL): PLC Code 3 (UL 746A)
Flame Characteristics
  • UL Recognized, 94V-0 Flame Class Rating: 1.5 mm (UL 94)
Injection Molding
  • Drying Temperature: 120°C
  • Drying Time: 3 – 4 hrs
  • Drying Time (Cumulative): 12 hrs
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 250 – 265°C
  • Nozzle Temperature: 245 – 260°C
  • Front Zone (Zone 3) Temperature: 250 – 265°C
  • Middle Zone (Zone 2) Temperature: 245 – 260°C
  • Rear Zone (Zone 1) Temperature: 240 – 255°C
  • Mold Temperature: 65 – 90°C
  • Back Pressure: 0.3 – 0.7 MPa
  • Screw Speed: 50 – 80 rpm
  • Shot to Cylinder Size: 40 – 80%
  • Vent Depth: 0.025 – 0.038 mm

Features & Benefits

Superior Flame Retardant Safety

VALOX 855 achieves a UL94 V-0 rating at just 1.5mm, ensuring critical fire safety in enclosed electrical devices and reducing risks in demanding applications.

Exceptional Heat & Dimensional Stability

With a Heat Deflection Temperature of 187°C at high stress, this resin maintains its shape and strength in high-heat environments like steam irons and oven components.

Excellent Processability & Aesthetics

VALOX™ FR resin 855 offers easy molding with high flow, leading to faster cycle times and superior surface quality for visible parts that also need to be durable.

15% glass filled valox fr pbt resin

Use & Application

  • Appliance Handles
  • Spotlights & Lighting Housings
  • Electric Motor Components
  • Pump Housings
15% glass filled valox fr pbt resin