Xenoy PC PBT 1102
XENOY™ Resin 1102 by SABIC is an unreinforced PC/polyester alloy engineered to deliver superior toughness and chemical resistance. It combines excellent low-temperature impact strength with resilience against automotive fluids, making it an ideal, durable choice for demanding components in harsh environments.
- Character: unreinforced PC/polyester alloy
Typical property data
Mechanical Properties
- Tensile Stress at Yield: 54 MPa
- Flexural Modulus: 1,960 MPa
- Flexural Stress at Yield: 82 MPa
Impact Properties
- Izod Impact, Notched (23°C): 800 J/m
- Izod Impact, Notched (-30°C): 640 J/m
Thermal Properties
- Heat Deflection Temp (1.82 MPa / 264 psi): 90 °C
Physical Properties
- Specific Gravity: 1.19
- Mold Shrinkage (Flow): 0.8 – 1.0%
Flame Performance
- UL Recognized
Processing Guidelines
- Drying: 110°C for 4-6 hours
- Melt Temperature: 260 – 275 °C
- Mold Temperature: 65 – 90 °C