Xenoy PC PBT 1102 Unreinforced PC Polyester Alloy
XENOY™ Resin 1102 by SABIC is an unreinforced PC/polyester alloy engineered to deliver superior toughness and chemical resistance. It combines excellent low-temperature impact strength with resilience against automotive fluids, making it an ideal, durable choice for demanding components in harsh environments.
Associated Documents
TDS Asia
TDS Americas
TDS Europe
XENOY™ Hospital Bed
Typical property data
Physical Properties
- Specific Gravity: 1.19 (ASTM D792)
- Specific Volume: 0.83 cm³/g (ASTM D792)
- Mold Shrinkage (Flow, 3.2 mm): 0.8 – 1% (SABIC Method)
- Mold Shrinkage (Crossflow, 3.2 mm): 0.8 – 1% (SABIC Method)
- Density: 1.19 g/cm³ (ISO 1183)
- Melt Volume Rate (MVR) at 250°C/2.16 kg: 6 cm³/10 min (ISO 1133)
Mechanical Properties
- Tensile Stress (Yield, 50 mm/min): 50 MPa (ISO 527)
- Tensile Stress (Break, 50 mm/min): 45 MPa (ISO 527)
- Tensile Strain (Yield, 50 mm/min): 4.5% (ISO 527)
- Tensile Strain (Break, 50 mm/min): 115% (ISO 527)
- Flexural Stress (Yield, 2 mm/min): 72 MPa (ISO 178)
- Flexural Modulus (2 mm/min): 1870 MPa (ISO 178)
Impact Properties
- Izod Impact (Notched, 80×10×4 mm, +23°C): 54 kJ/m² (ISO 180/1A)
- Izod Impact (Notched, 80×10×4 mm, 0°C): 52 kJ/m² (ISO 180/1A)
- Izod Impact (Notched, 80×10×4 mm, -30°C): 44 kJ/m² (ISO 180/1A)
Thermal Properties
- Heat Deflection Temperature (HDT), 0.45 MPa, 6.4 mm, Unannealed: 110°C (ASTM D648)
- Heat Deflection Temperature (HDT), 1.82 MPa, 6.4 mm, Unannealed: 90°C (ASTM D648)
- Heat Deflection Temperature (HDT/Af), 1.8 MPa, Flatw 80×10×4 mm: 79°C (ISO 75/Af)
Injection Molding
- Drying Temperature: 110°C
- Drying Time: 4 – 6 Hours (Cumulative: 8 Hours)
- Maximum Moisture Content: 0.02%
- Melt Temperature: 260 – 275°C
- Nozzle Temperature: 255 – 270°C
- Front Zone (Zone 3) Temperature: 255 – 275°C
- Middle Zone (Zone 2) Temperature: 250 – 270°C
- Rear Zone (Zone 1) Temperature: 245 – 265°C
- Mold Temperature: 65 – 90°C
- Back Pressure: 0.3 – 0.7 MPa
- Screw Speed: 50 – 80 rpm
- Shot to Cylinder Size: 50 – 80%
- Vent Depth: 0.013 – 0.02 mm
Features & Benefits
Exceptional Low-Temperature Toughness
XENOY™ Resin 1102 maintains high impact strength in cold environments, preventing brittle failure and ensuring part reliability for outdoor or refrigerated applications.
Resists Harsh Automotive Fluids
This alloy offers excellent resistance to oils, fuels, and greases, protecting components from degradation and extending service life in under-hood and fluid-handling systems.
Balanced Processability & Performance
XENOY 1102 provides a robust combination of mechanical properties and ease of molding, enabling the production of complex, durable parts efficiently and consistently.