Yulong A-2020 ABS Resin

yulong abs resin package

Yulong A-2020 General Purpose Grade

Yulong A-2020 is a high-performance ABS resin pellet offering excellent impact strength, rigidity, and thermal stability. It is widely suitable for injection molding processes, making it an ideal material choice for applications such as electronic housings, home appliances, and automotive components.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Melt Mass-Flow Rate (MFR): 19.1 g/10min (ASTM D1238)
  • Rockwell Hardness (R Scale): 111.0 (ASTM D785)
Mechanical Properties
    • Tensile Strength: 46.3 MPa (ASTM D638)
    • Nominal Strain at Tensile Break: 13.0% (ASTM D638)
    • Flexural Strength: 65.8 MPa (ASTM D790)
    • Flexural Modulus: 2400 MPa (ASTM D790)
Impact Properties
  • Notched Izod Impact Strength (1/4 inch): 21 kg-cm/cm (ASTM D256)
Thermal Properties
  • Vicat Softening Temperature (B50): 94.4°C (ASTM D1525)
Optical Properties
  • Yellowness Index: 8.0 (GB/T 39822-2021)
  • Whiteness: 59.2% (ASTM D313)

Features & Benefits

High Impact Resistance

Notched Izod impact strength of 21 kg·cm/cm helps prevent cracking during transport or use, extending product life.

Excellent Rigidity

Flexural modulus of 2400 MPa and Rockwell hardness of 111 ensure dimensional stability and strong load-bearing capacity, ideal for structural parts.

Excellent Processability

Melt flow rate of 19.1 g/10min enables easy injection molding with short cycle times, suitable for complex-shaped products.

yulong abs resin package

Use & Applications

  • Electronic device housings
  • Household appliance components
  • Automotive interior parts
  • Consumer goods and office equipment
  • Toys and sports equipment