Plastic Granules
Yulong Petrochemical S-0130
Yulong S-0130 AS Resin is a high-performance thermoplastic material offering exceptional mechanical strength, reliable thermal stability, and precise processing capabilities. Designed for demanding industrial applications, it is an ideal choice for robust and consistent production.
Typical property data
Physical Properties
- Large & Small Particles: ≤20 g/kg (SH/T 1541.1-2019)
- Impurities (count): 1 (Q/YLSH QM.02.063-2024)
- AN Content (Volume Fraction): 24.05% (Q/YLSH QM.02.074-2024)
Mechanical Properties
- Tensile Strength: 75.1 MPa (ASTM D638)
- Flexural Strength: 109 MPa (ASTM D790)
Thermal Properties
- Heat Deflection Temperature (Tf, 1.82 MPa): 87.3°C (ASTM D648)
Injection Molding
- Melt Mass-Flow Rate: 27.4 g/10min (10kg, 220°C) (ASTM D1238)
Features & Benefits
Outstanding Mechanical Strength
With a tensile strength of 75.1 MPa and flexural strength of 109 MPa, Yulong S-0130 resists deformation under stress. This ensures durable, long-lasting products ideal for structural and load-bearing applications such as automotive parts and consumer electronics.
Superb Thermal Stability
Featuring a heat deflection temperature of 87.3°C, Yulong S-0130 excels in high-temperature environments. This property makes it suitable for applications like electrical housings and industrial components exposed to elevated heat levels.
Efficient Processing Characteristics
Optimized for injection molding, Yulong S-0130 offers a melt mass-flow rate of 27.4 g/10min (ASTM D1238 at 220°C, 10 kg). This ensures smoother processing, precise finishes, and reduced manufacturing downtime.
Use & Applications
- Consumer Electronics
- Automotive
- Household Goods
- Industrial Equipment