Yuncon® CN90 POM Pellets Standard-flow Grade Acetal Copolymer
Yuncon® CN90 is a standard-flow POM copolymer resin. It offers high stiffness, high hardness, and low friction. MFR is 9 g/10 min. Tensile stress reaches 64 MPa. It suits gears, bearings, fittings, valves, wheels, and automotive parts.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Density: 1.41 g/cm³ (ISO 1183)
- Melt Mass-Flow Rate, MFR: 9 g/10 min at 190°C / 2.16 kg (ISO 1133)
- Water Absorption: 0.3% after 24 hr at 23°C (ISO 62)
Mechanical Properties
- Tensile Stress at Yield: 64 MPa (ISO 527-2)
- Tensile Modulus: 2600 MPa (ISO 527-2)
- Strain at Break: 30% (ISO 527-2)
- Flexural Strength: 88 MPa (ISO 178)
- Flexural Modulus: 2500 MPa (ISO 178)
- Charpy Notched Impact Strength: 6.0 kJ/m² (ISO 179/1eA)
Thermal Properties
- Heat Deflection Temperature: 95°C at 1.8 MPa, unannealed (ISO 75)
Flame Characteristics
- UL Flame Rating: HB class (UL 94)
Injection Molding Conditions
- Material Drying: 80–90°C for 3–4 hours
- Nozzle Temperature: 180–210°C
- Front Section Temperature: 190–210°C
- Center Section Temperature: 170–200°C
- Rear Section Temperature: 160–180°C
- Melt Temperature: 180–210°C
- Mold Temperature: 60–90°C
- Mold Temperature for Precision Parts: up to 120°C
- Injection Pressure: 50–100 MPa
- Holding Pressure: 30–80 MPa
- Back Pressure: 0–0.5 MPa
- Screw Rotational Speed: 50–120 rpm
Extrusion Conditions
- Recommended Extruder Type: Standard extruder with grooved feed zone and short compression screw
- Minimum Screw Length: 25D
- Extrusion Melt Temperature: 180–190°C
Use & Applications
- Automotive Electronics
- Automotive Exterior Parts
- Automotive Under-the-Hood Parts
- Bearings
- Fittings
- Gears
- Piping
- Pump Parts
- Thin-Walled Parts
- Valves / Valve Parts
- Wheels