Yuncon® M120 POM

yuntianhua acetal copolymer pom package

Yuncon® M120 POM Pellets Higher Flow Acetal Copolymer

Yuncon® M120 is a high-flow POM copolymer for injection molding. It offers 13 g/10 min MFR, 61 MPa tensile yield stress, and 2650 MPa tensile modulus. It provides low friction, good dimensional stability, and chemical resistance for gears, fittings, valves, and thin-wall parts.

Associated Documents

TDS - Data Sheet
UL Product id

Typical property data

Physical Properties
  • Density: 1.41 g/cm³ (ISO 1183)
  • Melt Mass-Flow Rate, MFR: 13 g/10 min at 190°C / 2.16 kg (ISO 1133)
  • Water Absorption: 0.3% after 24 hr at 23°C (ISO 62)
Mechanical Properties
  • Tensile Stress at Yield: 61 MPa (ISO 527-2)
  • Tensile Modulus: 2650 MPa (ISO 527-2)
  • Strain at Break: 30% (ISO 527-2)
  • Flexural Strength: 88 MPa (ISO 178)
  • Flexural Modulus: 2500 MPa (ISO 178)
  • Charpy Notched Impact Strength: 5.5 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature: 95°C at 1.8 MPa, unannealed (ISO 75)
Electrical Properties
  • Good electrical properties
Flame Characteristics
  • UL Flame Rating: HB class (UL 94)
Injection Molding Conditions
  • Material Drying Temperature: 80–90°C
  • Material Drying Time: 3–4 hours
  • Nozzle Temperature: 180–210°C
  • Front Section Temperature: 190–210°C
  • Center Section Temperature: 170–200°C
  • Rear Section Temperature: 160–180°C
  • Melt Temperature: 180–210°C
  • Mold Temperature: 60–90°C
  • Mold Temperature for Precision Parts: up to 120°C
  • Injection Pressure: 50–100 MPa
  • Holding Pressure: 30–80 MPa
  • Back Pressure: 0–0.5 MPa
  • Screw Rotational Speed: 50–120 rpm

Use & Applications

  • Automotive Electronics
  • Automotive Exterior Parts
  • Automotive Under-the-Hood Parts
  • Thin-Walled Parts
  • Fittings
  • Gears
  • Piping
  • Valves / Valve Parts
  • Wheels
yuntianhua acetal copolymer pom package