Typical property data

Physical Properties
  • Density: 1.41 g/cm³ (ISO 1183)
  • Melt Mass-Flow Rate, MFR: 9 g/10 min at 190°C / 2.16 kg (ISO 1133)
  • Water Absorption: 0.3% after 24 hr at 23°C (ISO 62)
Mechanical Properties
  • Tensile Stress at Yield: 61 MPa (ISO 527-2)
  • Tensile Modulus: 2600 MPa (ISO 527-2)
  • Strain at Break: 35% (ISO 527-2)
  • Flexural Strength: 90 MPa (ISO 178)
  • Flexural Modulus: 2600 MPa (ISO 178)
  • Charpy Notched Impact Strength: 6.0 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature: 95°C at 1.8 MPa, unannealed (ISO 75)
Flame Characteristics
  • UL Flame Rating: HB class (UL 94)
Injection Molding Conditions
  • Material Drying Temperature: 80–90°C
  • Material Drying Time: 3–4 hours
  • Nozzle Temperature: 180–210°C
  • Front Section Temperature: 190–210°C
  • Center Section Temperature: 170–200°C
  • Rear Section Temperature: 160–180°C
  • Melt Temperature: 180–210°C
  • Mold Temperature: 60–90°C
  • High-Precision Mold Temperature Option: Up to 120°C for precision parts
  • Injection Pressure: 50–100 MPa
  • Holding Pressure: 30–80 MPa
  • Back Pressure: 0–0.5 MPa
  • Screw Rotational Speed: 50–120 rpm
Extrusion Conditions
  • Extruder Type: Standard extruders with grooved feed zone
  • Screw Design: Short compression screw, minimum 25D
  • Extrusion Melt Temperature: 180–190°C

Use & Applications

  • Automotive Electronics
  • Automotive Exterior Parts
  • Automotive Under-the-Hood Components
  • Bearings
  • Fittings
  • Gears
  • Piping
  • Pump Parts
  • Thin-Walled Parts