Yuncon® N350 POM

yuntianhua acetal copolymer pom package

Yuncon® N350 POM Pellets Superhigh-flow Grade Acetal Copolymer

Yuncon® N350 is a superhigh-flow POM copolymer for injection molding. It has 35 g/10 min MFR, low mold deposit, and stable processing. It offers high hardness, low friction, good wear resistance, and chemical resistance for lighters, aerosol bottles, and fasteners.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Density: 1.41 g/cm³ (ISO 1183)
  • Melt Mass-Flow Rate, MFR: 35 g/10 min at 190°C/2.16 kg (ISO 1133)
  • Water Absorption: 0.5% at 24 hr, 23°C (ISO 62)
Mechanical Properties
  • Tensile Stress at Yield: 62 MPa (ISO 527-2)
  • Tensile Modulus: 2700 MPa (ISO 527-2)
  • Strain at Break: 20% (ISO 527-2)
  • Flexural Strength: 89 MPa (ISO 178)
  • Flexural Modulus: 2600 MPa (ISO 178)
  • Charpy Notched Impact Strength: 4.0 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature: 98°C at 1.8 MPa, unannealed (ISO 75)
Flame Characteristics
  • UL Flame Rating: HB class (UL 94)
Injection Molding Conditions
  • Material Drying Temperature: 80–90°C
  • Material Drying Time: 3–4 hours
  • Nozzle Temperature: 180–210°C
  • Front Section Temperature: 190–210°C
  • Center Section Temperature: 170–200°C
  • Rear Section Temperature: 160–180°C
  • Melt Temperature: 180–210°C
  • Mold Temperature: 60–90°C
  • Precision Parts Mold Temperature: Up to 120°C
  • Injection Pressure: 50–100 MPa
  • Holding Pressure: 30–80 MPa
  • Back Pressure: 0–0.5 MPa
  • Screw Rotational Speed: 50–120 rpm
Extrusion Conditions

Use & Applications

  • Lighters
  • aerosol bottles
  • fasteners
yuntianhua acetal copolymer pom package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.