Yuncon® N450 POM

yuntianhua acetal copolymer pom package

Yuncon® N450 POM Pellets Superhigh-flow Grade Acetal Copolymer

Yuncon® N450 is a superhigh-flow POM copolymer for injection molding. It has a high MFR of 45 g/10 min and minimized mold deposit. It offers low warpage, low friction, good abrasion resistance, and stable dimensions. Suitable for lighters, aerosol bottles, and fasteners.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Density: 1.41 g/cm³ (ISO 1183)
  • Melt Mass-Flow Rate, MFR at 190°C / 2.16 kg: 45 g/10 min (ISO 1133)
  • Water Absorption, 24 hr at 23°C: 0.3% (ISO 62)
Mechanical Properties
  • Tensile Stress at Yield: 62 MPa (ISO 527-2)
  • Tensile Modulus: 2750 MPa (ISO 527-2)
  • Strain at Break: 20% (ISO 527-2)
  • Flexural Strength: 89 MPa (ISO 178)
  • Flexural Modulus: 2600 MPa (ISO 178)
  • Charpy Notched Impact Strength: 3.5 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature, 1.8 MPa, Unannealed: 98°C (ISO 75)
Flame Characteristics
  • UL Flame Rating: HB class (UL 94)
Injection Molding Conditions
  • Material Drying Temperature: 80–90°C
  • Material Drying Time: 3–4 hours
  • Nozzle Temperature: 180–210°C
  • Front Cylinder Temperature: 190–210°C
  • Center Cylinder Temperature: 170–200°C
  • Rear Cylinder Temperature: 160–180°C
  • Melt Temperature: 180–210°C
  • Mold Temperature: 60–90°C
  • Mold Temperature for Precision Parts: Up to 120°C
  • Injection Pressure: 50–100 MPa
  • Holding Pressure: 30–80 MPa
  • Back Pressure: 0–0.5 MPa
  • Screw Rotational Speed: 50–120 rpm

Use & Applications

  • Lighters
  • Aerosol Bottles
  • Fasteners
yuntianhua acetal copolymer pom package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.