Plastic Granules
YUNGSOX® PP 1005 Homopolymer
YUNGSOX® PP 1005 is a premium homopolymer polypropylene resin designed for demanding manufacturing applications. With excellent melt strength and superior deep-drawing capabilities, it delivers reliable performance in thermoforming, blow molding, and pipe production.
Typical property data
Physical Properties
- Melt Index: 0.5 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
Mechanical Properties
- Tensile Strength at Yield: 370 kg/cm² (36 MPa) (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 300% (ISO 527 / ASTM D-638)
- Flexural Modulus: 15,500 kg/cm² (1520 MPa) (ISO 178 / ASTM D-790)
- Rockwell Hardness: 107 (R scale) (ISO 2039 / ASTM D-785)
Thermal Properties
- Heat Deflection Temperature: 117°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 155°C (ISO 306)
Processing Parameters
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications
- FDA Approval: Compliant with 21 CFR 177.1520, suitable for direct food contact.
- JHOSPA-PL Certification: Certified for compliance with Japanese JHOSPA-PL standards.
Use & Applications
- Thermoforming sheet
- PPH pipe