YUNGSOX® PP 1005N Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 1005N Homopolymer

YUNGSOX® PP 1005N is a versatile polypropylene homopolymer. With excellent melt strength, deep drawing capabilities, and good transparency, it ensures high performance in thermoforming and blow.

Associated Documents

TDS - Data Sheet
JCII Certification
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 0.5 g/10 min (ISO1133/ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO1183/ASTM D792)
Mechanical Properties
  • Tensile Strength at Yield: 360 Kg/cm² (35 MPa) (ISO527/ASTM D-638)
  • Tensile Elongation at Break: 300% (ISO527/ASTM D-638)
  • Rockwell Hardness: 105 (R scale) (ISO2039/ASTM D-785)
  • Flexural Modulus: 15,500 Kg/cm² (1520 MPa) (ISO178/ASTM D-790)
  • IZOD Impact Strength:
    • At 23°C: 45 Kg.cm/cm (441 J/m) (ISO180/ASTM D-256)
    • At -20°C: Unreported.
Thermal Properties
  • Heat Deflection Temperature: 115°C (ISO75/ASTM D-648)
  • Vicat Softening Temperature: 152°C (ISO306)
Processing Parameters
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications
  • FDA Approval: Complies with 21 CFR 177.1520
  • JHOSPA-PL Certification: Certified for compliance with Japanese JHOSPA-PL standards.

Use & Applications

  • Thermoforming sheet
  • Blow molding
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.