YUNGSOX® PP 1009 Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 1009 Homopolymer

YUNGSOX® PP 1009 is a high-performance polypropylene homopolymer resin. Engineered for excellent tensile strength and versatile applications, it is perfect for Thermoforming sheet, Blow molding, Strapping application.

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Use & Applications

  • Thermoforming sheet
  • Blow molding
  • Strapping
fpc taiwan polypropylene pp resin 25kg package

Typical property data

Physical Properties
  • Melt Index: 0.9 g/10 min (ISO 1133 / ASTM D1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
Mechanical Properties
  • Tensile Strength at Yield: 350 kg/cm² (34 MPa) (ISO 527 / ASTM D638)
  • Tensile Elongation at Break: 300% (ISO 527 / ASTM D638)
  • Flexural Modulus: 13,500 kg/cm² (1324 MPa) (ISO 178 / ASTM D790)
  • Rockwell Hardness (R Scale): 105 (ISO 2039 / ASTM D785)
Thermal Properties
  • Melting Point: Not specified
  • Heat Deflection Temperature: 115°C (ISO 75 / ASTM D648)
  • Vicat Softening Temperature: 152°C (ISO 306)
Processing Parameters
  • Mold Shrinkage: 1.3–1.7% (FPC Method)