Plastic Granules
YUNGSOX® PP 1020L Homopolymer
YUNGSOX® PP 1020L is a premium-grade homopolymer polypropylene resin. With its excellent tensile strength, thermal stability, and FDA compliance for food contact safety. Designed for demanding industrial applications, it combines lightweight durability with superior processing performance.
Typical property data
Physical Properties
- Melt Index: 1.7 g/10min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D-792)
Mechanical Properties
- Tensile Strength at Yield: 34 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 400% (ISO 527 / ASTM D-638)
- Flexural Modulus: 1324 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness (R Scale): 105 (ISO 2039 / ASTM D-785)
Thermal Properties
- Heat Deflection Temperature: 115°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 152°C (ISO 306)
Processing Parameters
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Use & Applications
- Pressure forming sheet
- Portfolio
- Bottles
- Strapping