Typical property data

Physical Properties
  • Melt Index (ISO 1133 / ASTM D1238): 2.8 g/10 min
  • Density (ISO 1183 / ASTM D792): 0.91 g/cm³
Mechanical Properties
  • Tensile Strength at Yield (ISO 527 / ASTM D638): 350 kg/cm² (34 MPa)
  • Tensile Elongation at Break (ISO 527 / ASTM D638): 400%
  • Rockwell Hardness (R Scale, ISO 2039 / ASTM D785): 105
  • Flexural Modulus (ISO 178 / ASTM D790): 13,500 kg/cm² (1324 MPa)
  • IZOD Impact Strength at 23°C (ISO 180 / ASTM D256): 7 kg.cm/cm (69 J/m)
Thermal Properties
  • Heat Deflection Temperature (ISO 75 / ASTM D648): 105°C
  • Vicat Softening Temperature (ISO 306): 150°C
Processing Parameters
  • Mold Shrinkage (FPC Method): 1.3–1.7%

Use & Applications

  • Transparency pressure forming sheet
  • Portfolio
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.