YUNGSOX® 1024 is a premium-grade homopolymer polypropylene resin. With its high stiffness, excellent transparency, superior heat resistance, and low n-hexane extractability, Engineered for precision and safety, it meets stringent regulatory standards. Ideal for Transparent pressure forming sheet, Portfolio, Bottles.
Associated Documents
TDS - Data Sheet
USP Class VI
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH
Typical property data
Physical Properties
- Melt Index (ISO 1133 / ASTM D-1238): 1.8 g/10min
- Density (ISO 1183 / ASTM D792): 0.91 g/cm³
- Mold Shrinkage (FPC Method): 1.3–1.7%
Mechanical Properties
- Tensile Strength at Yield (ISO 527 / ASTM D-638): 400 Kg/cm² (39 MPa)
- Tensile Elongation at Break (ISO 527 / ASTM D-638): 200%
- Flexural Modulus (ISO 178 / ASTM D-790): 16,000 Kg/cm² (1569 MPa)
- Rockwell Hardness – R Scale (ISO 2039 / ASTM D-785): 110
- IZOD Impact Strength (ISO 180 / ASTM D-256):
- At 23°C: 6 Kg.cm/cm (59 J/m)
- At -20°C: Not available
Thermal Properties
- Melting Point (DSC): Not specified
- Vicat Softening Temperature (ISO 306): 155°C
- Heat Deflection Temperature (ISO 75 / ASTM D-648): 122°C
Certifications
- FDA Compliance: FDA 21 CFR 177.1520 regulations
- Biocompatibility: Compliant with USP Class VI Biological Reactivity Tests
Use & Applications
- Blow-molded bottles used in food, beverages, and household products
- Liquid medicine bottles
- Eye drop bottles