YUNGSOX® PP 1024T is a high-performance homopolymer polypropylene resin. It offers exceptional transparency, high stiffness, and remarkable heat resistance. Applications: Transparency pressure forming sheet and Portfolio.
Typical property data
Physical Properties
- Density: 0.91 g/cm³ (ISO 1183 | ASTM D792)
- Melt Index: 1.8 g/10min (ISO 1133 | ASTM D1238)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 380 kg/cm² (37 MPa) (ISO 527 | ASTM D638)
- Tensile Elongation at Break: 200% (ISO 527 | ASTM D638)
- Flexural Modulus: 15,000 kg/cm² (1471 MPa) (ISO 178 | ASTM D790)
- Rockwell Hardness: 110 (R Scale) (ISO 2039 | ASTM D785)
- IZOD Impact Strength (23°C): 6 kg.cm/cm (59 J/m) (ISO 180 | ASTM D256)
Thermal Properties
- Vicat Softening Temperature: 153°C (ISO 306)
- Heat Deflection Temperature: 120°C (ISO 75 | ASTM D648)