Plastic Granules
YUNGSOX® PP 1025 Homopolymer
YUNGSOX® PP 1025 Homopolymer PP Plastic Resin delivers exceptional performance with a unique blend of good transparency, high stiffness, and superior heat resistance. Applications: Transparency pressure forming sheet, Portfolio, Bottles.
Typical property data
Physical Properties
- Melt Index: 1.8 g/10min (ISO 1133 / ASTM D-1238)
- Density: 0.91 g/cm³ (ISO 1183 / ASTM D792)
Mechanical Properties
- Tensile Strength at Yield: 400 Kg/cm² (39 MPa) (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 200% (ISO 527 / ASTM D-638)
- Flexural Modulus: 16,000 Kg/cm² (1569 MPa) (ISO 178 / ASTM D-790)
- Rockwell Hardness: 110 R scale (ISO 2039 / ASTM D-785)
- IZOD Impact Strength (Notch, 23°C): 6 Kg.cm/cm (59 J/m) (ISO 180 / ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 122°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 155°C (ISO 306)
Processing Parameters
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Regulatory Approvals
- FDA Approval: with FDA 21 CFR 177.1520 regulations
Use & Applications
- Transparency pressure forming sheet
- Portfolio
- Bottles