Plastic Granules
YUNGSOX® PP 1030T Homopolymer
YUNGSOX® PP 1030T offers excellent transparency, high stiffness, and superior heat resistance. This premium material ensures durability and clarity. Ideal for Transparency pressure forming sheet and Portfolio applications.
Typical property data
Physical Properties
- Melt Index: 3.0 g/10min (ISO 1133 / ASTM D1238)
- Density: 0.91 g/cm³ (ISO 1183 / ASTM D792)
Mechanical Properties
- Tensile Strength at Yield: 350 kg/cm² (34 MPa) (ISO 527 / ASTM D638)
- Tensile Elongation at Break: 400% (ISO 527 / ASTM D638)
- Flexural Modulus: 14,000 kg/cm² (1373 MPa) (ISO 178 / ASTM D790)
- Rockwell Hardness: 105 (R scale) (ISO 2039 / ASTM D785)
- Izod Impact Strength:
- At 23°C: 8 kg.cm/cm (78 J/m) (ISO 180 / ASTM D256)
- At -20°C: Data unavailable
Thermal Properties
- Heat Deflection Temperature: 105°C (ISO 75 / ASTM D648)
- Vicat Softening Temperature: 150°C (ISO 306)
Processing Parameters
- Mold Shrinkage: 1.3–1.7% (Tested by FPC Method)
Certifications & Compliance
- FDA Approval: FDA requirements (21 CFR 177.1520)
- JHOSPA-PL Certification: Certified by JHOSPA-PL standards
Use & Applications
- Transparency pressure forming sheet
- Portfolio