YUNGSOX® PP 1040 Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 1040 Homopolymer

YUNGSOX® PP 1040 is a high-performance homopolymer polypropylene resin. It offers excellent heat resistance and superior stiffness, making it ideal for toys, electrical appliances, and durable housewares.

Associated Documents

TDS - Data Sheet
PL JCII Certification
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 5 g/10min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
Mechanical Properties
  • Tensile Strength at Yield: 350 Kg/cm² (34 MPa) (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 550% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 14,000 Kg/cm² (1373 MPa) (ISO 178 / ASTM D-790)
  • Rockwell Hardness: R Scale 105 (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength (Notched):
    • At 23°C: 4.0 Kg.cm/cm (39 J/m) (ISO 180 / ASTM D-256)
    • At -20°C: Not available
Thermal Properties
  • Heat Deflection Temperature: 115°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 155°C (ISO 306)
Processing Parameters
  • Mold Shrinkage: 1.3 – 1.7% (FPC Method)
Certifications & Compliance
  • FDA Compliance: 21 CFR 177.1520
  • UL Certification: UL 94HB certified
  • JHOSPA-PL Certification: Certified for compliance with Japanese safety standards

Use & Applications

  • General purpose
  • Toys
  • Electrical appliances
  • Housewares