YUNGSOX® PP 1040U Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 1040U Homopolymer

YUNGSOX® PP 1040U, a premium-grade polypropylene homopolymer, offers outstanding weather resistance and superior tensile strength. Designed for Yarn and Monofilament applications, it ensures durability, efficiency, and performance.

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index (ISO 1133): 3 g/10min
  • Density (ISO 1183): 0.90 g/cm³
Mechanical Properties
  • Tensile Strength at Yield (ISO 527): 350 kg/cm²
  • Tensile Elongation at Break (ISO 527): 600%
  • Rockwell Hardness (ISO 2039): 105 R Scale
  • Flexural Modulus (ISO 178): 12,500 kg/cm²
Thermal Properties
  • Heat Deflection Temperature (ISO 75): 113°C
  • Vicat Softening Temperature (ISO 306): 150°C
Processing Parameters
  • Mold Shrinkage (FPC Method): 1.3–1.7%

Use & Applications

  • Yarn-Based Solutions

    • Woven Bags
    • Carpet Backing
  • Monofilament Products

    • Brush Filaments
    • Rope Manufacturing