Typical property data

Physical Properties
  • Melt Index: 10 g/10min (ISO 1133 / ASTM D1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
Mechanical Properties
  • Tensile Strength at Yield: 350 kg/cm² (34 MPa) (ISO 527 / ASTM D638)
  • Tensile Elongation at Break: 500% (ISO 527 / ASTM D638)
  • Rockwell Hardness: 107 (R Scale) (ISO 2039 / ASTM D785)
  • Flexural Modulus: 14,000 kg/cm² (1373 MPa) (ISO 178 / ASTM D790)
  • Izod Impact Strength (23°C): 3.5 kg·cm/cm (34 J/m) (ISO 180 / ASTM D256)
Thermal Properties
  • Heat Deflection Temperature: 115°C (ISO 75 / ASTM D648)
  • Vicat Softening Temperature: 155°C (ISO 306)
Flame Characteristics
  • UL Certification: UL 94HB
Processing Parameters
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Approval: Complies with 21 CFR 177.1520 for food contact.
  • JHOSPA-PL Certification: Certified under Japanese JHOSPA-PL standards.
  • UL Certification: UL 94HB for flammability.

Use & Applications

  • General purpose
  • Food containers
  • Electrical appliances
  • Housewares
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.