Physical Properties
- Melt Index: 11 g/10 min (ISO 1133/ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183/ASTM D792)
Mechanical Properties
- Tensile Strength at Yield: 380 kg/cm² (37 MPa) (ISO 527/ASTM D-638)
- Tensile Elongation at Break: 500% (ISO 527/ASTM D-638)
- Flexural Modulus: 14,500 kg/cm² (1422 MPa) (ISO 178/ASTM D-790)
- Rockwell Hardness: R scale, 107 (ISO 2039/ASTM D-785)
- IZOD Impact Strength (23°C): 3.5 kg/cm² (34 MPa) (ISO 180/ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 115°C (DSC)
- Vicat Softening Temperature: 155°C (ISO 75/ASTM D-648)
Processing Parameters
- Mold Shrinkage: 1.3–1.7% (FPC Method)