YUNGSOX® 1124 Homopolymer
YUNGSOX® PP 1124 is a high-performance polypropylene homopolymer. Key Features: High Heat Resistance, Exceptional Stiffness, Abrasion Resistance, Good Luster. Ideal for Electrical appliances, Microwave food containers, Housewares applications.
Associated Documents
TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH
Typical property data
Physical Properties
- Melt Index: 15 g/10 min (ISO 1133/ASTM D-1238)
- Density: 0.91 g/cm³ (ISO 1183/ASTM D792)
Mechanical Properties
- Tensile Strength at Yield: 490 Kg/cm² (48 MPa) (ISO 527/ASTM D-638)
- Tensile Elongation at Break: 50% (ISO 527/ASTM D-638)
- Flexural Modulus: 22,000 Kg/cm² (2157 MPa) (ISO 178/ASTM D-790)
- Rockwell Hardness: 115 (R Scale) (ISO 2039/ASTM D-785)
- IZOD Impact Strength:
- At 23°C: 3.0 Kg·cm/cm (29 J/m) (ISO 180/ASTM D-256)
- At -20°C: Data not provided
Thermal Properties
- Vicat Softening Temperature: 157°C (ISO 306)
- Heat Deflection Temperature: 135°C (ISO 75/ASTM D-648)
Processing Parameters
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
- Certified to comply with FDA 21 CFR 177.1520, allowing safe use in food contact applications.
Use & Applications
- Electrical Appliances
- Microwave Food Containers
- Housewares