YUNGSOX® PP 1124H Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® 1124H Homopolymer Superior Heat Resistance

YUNGSOX® PP 1124H is a Homopolymer polypropylene resin with FDA Approval. Designed for electrical appliances, microwave food containers, and housewares. It features long-term heat resistance, excellent abrasion resistance, and good luster. High stiffness making it suitable for structural applications.

Associated Documents

TDS - Data Sheet
PL JCII Certification
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 23 g/10 min (ISO1133 / ASTM D-1238)
  • Density: 0.91 g/cm³ (ISO1183 / ASTM D792)
Mechanical Properties
  • Tensile Strength at Yield: 470 kg/cm² (46 MPa) (ISO527 / ASTM D-638)
  • Tensile Elongation at Break: 50% (ISO527 / ASTM D-638)
  • Rockwell Hardness (R Scale): 111 (ISO2039 / ASTM D-785)
  • Flexural Modulus: 17000 kg/cm² (1667 MPa) (ISO178 / ASTM D-790)
  • IZOD Impact Strength (Notch):
    • At 23°C: 3.0 kg·cm/cm (29 J/m) (ISO 180 / ASTM D-256)
    • At -20°C: Data not available
Thermal Properties
  • Heat Deflection Temperature: 120°C (ISO75 / ASTM D-648)
  • Vicat Softening Temperature: 155°C (ISO306)
Flame Characteristics
  • UL Certification: UL 94HB Flame Resistance
  • Relative Temperature Index (RTI): 125°C (UL746B)
Processing Parameters
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Approval: Complies with CFR 21 177.1520 regulations for direct food contact.
  • UL Certification: UL 94HB, UL746B RTI 125°C.
  • JHOSPA-PL Certification: Approved under Japanese standards.

Use & Applications

  • Electrical appliances
  • Microwave food containers
  • Housewares
fpc taiwan polypropylene pp resin 25kg package