YUNGSOX® 1202F Homopolymer Superior Anti-gas-fading
YUNGSOX® PP 1202F is a high-performance polypropylene homopolymer resin. It features exceptional anti-gas fading, superior stretchability, and excellent tensile strength. This grade is widely used in applications such as geotextiles, industrial textiles, carpet facing, and woven tapes.
Associated Documents
TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH
Typical property data
Physical Properties
- Melt Index (MI): 18 g/10 min (ISO 1133 | ASTM D1238)
- Density: 0.90 g/cm³ (ISO 1183 | ASTM D792)
Mechanical Properties
- Tensile Strength at Yield: 350 kg/cm² (34 MPa) (ISO 527 | ASTM D638)
- Tensile Elongation at Break: 300% (ISO 527 | ASTM D638)
- Flexural Modulus: 13,500 kg/cm² (1,324 MPa) (ISO 178 | ASTM D790)
- Rockwell Hardness: 105 (R Scale) (ISO 2039 | ASTM D785)
- IZOD Impact Strength (23°C): 3 kg·cm/cm (29 J/m) (ISO 180 | ASTM D256)
Thermal Properties
- Heat Deflection Temperature: 115°C (ISO 75 | ASTM D648)
- Vicat Softening Temperature: 152°C (ISO 306)
Processing Parameters
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
- FDA Approval: Compliant with FDA requirements under 21 CFR 177.1520, safe for direct food contact.
Use & Applications
- Geotextiles for soil reinforcement.
- Textiles in industrial and construction usage.
- Carpet facings for enhanced durability and aesthetics.
- Woven tapes, offering superior stretch and strength.