Plastic Granules
YUNGSOX® 1250D Homopolymer
YUNGSOX® PP 1250D is a homopolymer polypropylene (PP) resin from Formosa Plastics Corporation, designed for thin-wall injection molding, storage boxes, and houseware applications. The grade provides high fluidity, good luster, and low warpage, making YUNGSOX® PP 1250D suitable for high-productivity molding of rigid consumer and industrial plastic parts.
Associated Documents
TDS - Data Sheet
USP Class VI
PL JCII Certification
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH
Typical property data
Physical Properties
Melt Index: 25 g/10 min (ISO 1133 / ASTM D-1238)
Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
Tensile Strength at Yield:400 kg/cm² / 39 MPa (ISO 527 / ASTM D-638)
Tensile Elongation at Break:50% (ISO 527 / ASTM D-638)
Rockwell Hardness:R111 (ISO 2039 / ASTM D-785)
Flexural Modulus:16,000 kg/cm² / 1,569 MPa (ISO 178 / ASTM D-790)
IZOD Impact Strength, 23°C:3.0 kg·cm/cm / 29 J/m (ISO 180 / ASTM D-256)
IZOD Impact Strength,-20°C (ISO 180 / ASTM D-256
Thermal Properties
- Heat Deflection Temperature: 120°C (ISO 75 / ASTM D-648)
Vicat Softening Temperature: 155°C (ISO 306)
Processing Parameters
Melt Index: 25 g/10 min (ISO 1133 / ASTM D-1238)
Mold Shrinkage: 1.3–1.7% (FPC Method)
Processing Feature:High fluidity
Warpage Performance:Low warpage
Use & Applications
- Thin walled products
- Storage boxes
- Housewares