YUNGSOX® PP 1350D Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® 1350D Homopolymer

YUNGSOX® PP 1350D is a high-fluidity homopolymer PP resin for thin-wall injection molding. It delivers good luster, low warpage, and stable molding performance for storage boxes, housewares, and rigid consumer products.

Associated Documents

TDS - Data Sheet
PL JCII Certification
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 35 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 400 kg/cm² / 39 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 50% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: 111 R scale (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 16,000 kg/cm² / 1,569 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched, 23°C: 3.0 kg·cm/cm / 29 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength, Notched, -20°C: (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 120°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 155°C (ISO 306)
Optical Properties
  • Luster: Good luster
Processing Parameters
  • Processing Method: Injection Molding
  • Recommended Application Type: Thin-Walled Products
  • Flow Characteristic: High Fluidity
  • Warpage Characteristic: Low Warpage
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520
  • JHOSPA-PL Certification

Use & Applications

  • Thin walled products
  • Storage boxes
  • Housewares
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.