YUNGSOX® PP 1352F Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 1352F Homopolymer

YUNGSOX® PP 1352F is a homopolymer PP resin for non-woven fabrics, filter cloth, and industrial textiles. It offers anti gas-fading performance, good stretchability, and soft hand feel.

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 35 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 300 kg/cm² / 29 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 100% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: R105 (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 13,000 kg/cm² / 1,275 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched, 23°C: 3 kg·cm/cm / 29 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength, Notched, -20°C: (ISO 180 / ASTM D-256)
Thermal Properties
  • Melting Point: (DSC)
  • Heat Deflection Temperature: 115°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 152°C (ISO 306)
Processing Parameters
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Food Contact Compliance: under 21 CFR 177.1520

Use & Applications

  • Non-woven fabric
  • Filter cloth
  • Industrial textile