YUNGSOX® PP 1600D Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 1600D Homopolymer

YUNGSOX® PP 1600D is a homopolymer PP resin for high-speed thin-wall injection molding. It delivers superhigh fluidity, fast cycling, good luster, and low warpage for efficient production and clean finished parts.

Associated Documents

TDS - Data Sheet
PL JCII Certification
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 60 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 380 kg/cm² / 37 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 50% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: 110 R scale (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 15,500 kg/cm² / 1,520 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched, 23°C: 3.0 kg·cm/cm / 29 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength, Notched, -20°C:
Thermal Properties
  • Heat Deflection Temperature: 118°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 153°C (ISO 306)
Processing Parameters
  • Recommended Processing: High-speed thin-wall injection molding
  • Flow Performance: Superhigh fluidity
  • Cycle Performance: Fast cycling
  • Dimensional Performance: Low warpage
  • Surface Appearance: Good luster
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520 for direct food contact
  • JHOSPA-PL Certification

Use & Applications

  • High speed thin walled injection molding products
  • Storage boxes
  • Housewares