YUNGSOX® PP 1600N Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® 1600N PP Homopolymer

YUNGSOX® PP 1600N is a premium homopolymer polypropylene resin with superhigh fluidity, excellent luster, and low warpage. Ideal for thin-walled products, it ensures precision, durability, and an attractive finish for high-performance applications.

Associated Documents

TDS - Data Sheet
PL JCII Certification
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 60 g/10min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 400 kg/cm² (39 MPa) (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 50% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 17,000 kg/cm² (1667 MPa) (ISO 178 / ASTM D-790)
  • Rockwell Hardness: 111 (R scale) (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength (23°C): 3.6 kg.cm/cm notch (35 J/m) (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 125°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 155°C (ISO 306)
Certifications & Compliance
  • FDA Approval: U.S. FDA requirements under 21 CFR 177.1520 for food contact.
  • JHOSPA-PL Certification

Use & Applications

  • Thin walled products
  • Storage boxes